ASTM B167 Uns N06600 2.4816 Inconel 600 Nickel Alloy Tubing introduction

ASTM B167 Uns N06600 2.4816 Inconel 600 Nickel Alloy Tubing introduction
ASTM B167 UNS N06600 2.4816 Inconel 600 is a high-nickel-chromium iron alloy tubing known for its excellent resistance to high temperatures, a wide range of chemicals, and corrosion, particularly chloride ions and alkaline solutions. Its strong mechanical properties and good processing characteristics make it a versatile material suitable for demanding applications such as heat treating, nuclear reactors, chemical processing, and aerospace components.
What is the ASTM standard for Inconel 600?
Inconel 600 round bar is composed of 72% nickel, 14% chromium, iron, carbon, manganese, sulfur, silicon, and copper. This material has a high melting point of 1413°C. The minimum yield strength of ASTM B166 UNS N06600 round bar is 310 MPa, and the minimum tensile strength is 655 MPa.

Uns N06600 2.4816 Inconel 600 Nickel Alloy Tubing Chemical Composition
| UNS Designation | N06600 |
| Inconel Alloy | 600 |
| Nickel (+ Cobalt) | 72 min. |
| Cromium | 14.0 - 17.0 |
| Iron | 6.00 - 10.00 |
| Carbon | 0.15 max. |
| Manganese | 1.0 max. |
| Sulfur | 0.015 max. |
| Silicon | 0.50 max |
| Copper | 0.50 max. |
Uns N06600 2.4816 Inconel 600 Tubing Mechanical Properties
| Product Form | Condition | Tensile (ksi) | .2% Yield (ksi) | Elongation (%) | Hardness (HRB) |
| Tube & Pipe | ot-Finished | 75-100 | 25-50 | 35*55 | - |
| Tube & Pipe | Cold-Drawn | 80-100 | 25-50 | 35-55 | 88 Max |
Uns N06600 2.4816 600 Nickel Alloy Tubing Equivalent Material
| Grade | UNS No | Old British | Euronorm | GOST | Japanese JIS | ||
| BS | En | No | AFNOR | ||||
| Inconel 600 | N06600 | NA 13 | NiCr15Fe | 2.4816 | NC15FE11M | МНЖМц 28-2,5-1,5 | NCF 600 |
Inconel 600 Nickel Alloy Tubing Material Composition and Key Properties
Composition: Inconel 600 tubing is a nickel-chromium alloy with a high nickel content (at least 72%), a relatively high chromium content (14-17%), and an iron content of approximately 6-10%.
Corrosion Resistance: The high nickel content provides excellent resistance to chloride stress corrosion cracking and alkaline environments, while the chromium content enhances its resistance to oxidizing environments and sulfur-containing compounds.
Mechanical Strength: The alloy's high strength and good workability make it suitable for high-stress and high-temperature applications.
Temperature Range: It performs well in temperatures ranging from cryogenic to high temperatures up to 2000°F (1093°C).
Inconel 600 Nickel Alloy Tubing Applications
Due to its unique properties, ASTM B167 Inconel 600 tubing is widely used in a variety of industries:
Chemical Processing: Equipment used to handle various organic and inorganic compounds, fatty acids, and certain corrosive environments. High-Temperature Applications: Widely used for heat treatment of components such as stills, muffle furnaces, and furnace components.
Nuclear Industry: Due to its excellent resistance to high-purity water and its resistance to chloride-ion stress corrosion cracking, it is a standard manufacturing material for nuclear reactor components.
Aerospace: Suitable for high-temperature engine and airframe components, such as exhaust liners and turbine seals.
Marine Applications: Due to its resistance to corrosive environments, it can be used in seawater and marine applications.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.