Astm B167 Inconel 600 High Resistance Heat Exchanger Seamless Tube
Gnee Steel
Astm B167 Inconel 600 High Resistance Heat Exchanger Seamless Tube
ASTM B167 specifies the use of Inconel 600 tubing (UNS N06600), a nickel-iron-chromium alloy with excellent high-temperature strength and resistance to oxidation, scaling, and chloride stress corrosion cracking. This makes it ideal for heat exchanger tubing used in demanding, corrosive, and high-temperature environments such as chemical processing, nuclear reactors, and heat-treating furnaces. Seamless tubing is widely used due to its excellent mechanical properties and stability in high-pressure applications.

Gnee Steel
What are the standard Inconel 600 pipes?
These pipes conform to ASTM B167, B829, and B517 specifications. Pipes are available in various sizes according to ASTM, ASME, and API standards. Inconel 600 seamless pipes are available in diameters from 4 mm to 219 mm, while welded and EFW pipes are available in diameters from 5 mm to 1219.2 mm, with wall thicknesses ranging from 0.5 mm to 20 mm.

Specification Chart of Inconel 600 Pipe
| ASTM Specification | ASTM B 167 ASME SB 167 / ASTM B 829 ASME SB 829 / ASTM B 517 ASME SB 517 |
|---|---|
| Standard | ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB |
| ASTM B167 inconel 600 Seamless Pipe Size | 4 to 219mm W. T.: 0.5 to 20mm |
| UNS N06600 Welded Pipe Size | 5.0 - 1219.2 mm |
| Inconel WERKSTOFF NR. 2.4816 EFW Pipe size | 5.0 - 1219.2 mm |
| Swg & Bwg | 12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg., |
| 600 Inconel Pipe Schedule | XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160 |
| inconel 600 pipe Length | Double Random, Single Random, Standard & Cut length Pipe |
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc |
Inconel 600 High Resistance Heat Exchanger Seamless Tube Materials and Properties
High Temperature Resistance: Due to its high melting point and thermal stability, it maintains structural integrity and mechanical strength at high temperatures.
Corrosion Resistance:
Excellent resistance to dry chlorine and hydrogen chloride corrosion.
Resists oxidation and scaling, forming a protective oxide layer at high temperatures.
Stable in both acidic and alkaline environments.
600 Tubing Applications in Heat Exchangers
Operating Environment: Suitable for high temperature, high pressure, and corrosive environments.
Specific Applications:
Nuclear reactors and related heat exchangers.
Chemical processing equipment, particularly those involving chlorine, hydrogen fluoride, and alkali metals.
Heat treatment furnaces, including applications in carburizing and nitriding environments.
Petrochemical production and hot working.
Standards and Manufacturing
Standard: ASTM B167 specifies the requirements for Inconel 600 seamless nickel-chromium-iron alloy tubing. Seamless Tubing: Manufactured seamlessly (without welds), these tubings offer exceptional reliability for demanding applications such as boilers and heat exchangers.
Testing: Alloys undergo chemical analysis, tensile testing, and hydrostatic or nondestructive electrical testing to ensure compliance with standards.
ASTM B167 Inconel 600 seamless pipe Sizes
| ASTM B167 inconel 600 Pipe OD mm |
Pipe WT mm |
in. | Sch | Kg/m |
|---|---|---|---|---|
| 13.72 | 1.65 | 1/4 | 10S | 0.50 |
| 13.72 | 2.24 | 1/4 | 40S | 0.64 |
| 13.72 | 3.02 | 1/4 | 80S | 0.81 |
| 17.15 | 1.65 | 3/8 | 10S | 0.64 |
| 17.15 | 2.31 | 3/8 | 40S | 0.86 |
| 17.15 | 3.20 | 3/8 | 80S | 1.12 |
| 21.34 | 2.11 | 1/2 | 10S | 1.02 |
| 21.34 | 2.77 | 1/2 | 40S | 1.29 |
| 21.34 | 3.73 | 1/2 | 80S | 1.65 |
| 26.67 | 2.11 | 3/4 | 10S | 1.30 |
| 26.67 | 2.87 | 3/4 | 40S | 1.71 |
| 26.67 | 3.91 | 3/4 | 80S | 2.23 |
| 33.40 | 2.77 | 1 | 10S | 2.13 |
| 33.40 | 3.38 | 1 | 40S | 2.54 |
| 33.40 | 4.55 | 1 | 80S | 3.29 |
| 33.40 | 6.352) | 1 | 160 | 4.30 |

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications, and we can provide customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneemetal.com.