ASME SB622 UNS N10276 Hastelloy C276 Chemical Processing Pipe

 
ASME SB622 UNS N10276 Hastelloy C276 Chemical Processing Pipe
 

Gnee Steel

 

ASME SB622 UNS N10276 Hastelloy C276 Chemical Processing Pipe

ASME SB622 UNS N10276 Hastelloy C276 is a nickel-based high-temperature alloy pipe designed for exceptional corrosion resistance in harsh chemical processing environments. It is renowned for its resistance to oxidizing and reducing acids, chlorides, and other corrosive media. The alloy's low carbon content prevents carbide precipitation at grain boundaries during welding, maintaining corrosion resistance in the heat-affected zone of welded joints. Due to its exceptional strength and formability, this pipe is widely used in demanding applications such as chemical processing equipment, pollution control systems, and marine environments.

Hastelloy C276 Chemical Processing Pipe

Gnee Steel

 

What are the specifications for Hastelloy C276 pipe?

This composition gives the material a high melting point of 1370°C. Hastelloy C276 seamless pipe has a minimum yield strength of 355 MPa and a minimum tensile strength of 790 MPa. The material also has a high density of 8.89 grams per cubic centimeter.

Hastelloy C276 pipe

Hastelloy C276 Tubes Specifications

 

Specifications ASTM B619, B622 / ASME SB619, SB622
Dimensions ASTM, ASME and API
Size 6 mm OD x 0.7 mm to 50.8 mm OD x 3 mm thk.
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Type Seamless / ERW / Welded / Fabricated / LSAW Tubes
Form Round Tubes, Custom Tubes, Square Tubes, Rectangular Tubes, "U" Shape, Hydraulic Tubes
Length Single Random, Double Random & Cut Length.
End Plain End, Beveled End, Treaded

 

C276 Hastelloy Pipe Chemical Composition

Ni C Mo Mn Si Fe P S Co Cr
Balance 0.01 max 15 - 17 1.0 max 0.08 max 4 - 7 0.04 max 0.03 max 2.5 max 14.5 - 16.5

 

Equivalent Grades of Hastelloy Alloy C276 Tubes

STANDARD UNS WNR. AFNOR EN JIS OR GOST
Hastelloy C276 N10276 2.4819 - NiMo16Cr15W NW 0276 ЭП760 ХН65МВУ

 

ASTM B622 Hastelloy C276 Seamless Pipes Physical Properties

Properties

Metric

Imperial

Density 8.89 g/cm³ 0.321 lb/in³
Melting point 1371°C 2500°F

 

Key Features
Excellent Corrosion Resistance: Provides excellent corrosion resistance in both oxidizing and reducing environments, including strong acids, ferric and cupric chlorides, and wet chlorine.
High Nickel and Molybdenum Content: These elements provide excellent corrosion resistance in reducing environments.
Low Carbon Content: Minimizes carbide precipitation during welding, maintaining corrosion resistance in the weld area.
Localized Corrosion Resistance: Effectively protects against pitting, crevice corrosion, and stress corrosion cracking.
High-Temperature Mechanical Properties: Demonstrates strong mechanical durability at high temperatures.

 

Applications
Chemical Processing: Widely used in chemical plants handling corrosive media such as acids and chloride solutions.
Pollution Control: Suitable for use in pollution control system components such as scrubbers, dampers, and flue gas reheaters.
Industrial Waste Treatment: Used in industrial and municipal waste treatment systems.
Pulp and Paper Production: Valued in processes within the pulp and paper industry.
Marine Environments: Its excellent corrosion resistance makes it ideal for marine applications and salty seawater.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.