ASME SB163 UNS N04400 Nickel Alloy U-Bend Pipe

ASME SB163 UNS N04400 Nickel Alloy U-Bend Pipe
ASME SB163 UNS N04400 nickel alloy U-bends are heat exchanger tubes made from Monel 400 alloy, known for its excellent resistance to high-temperature steam, seawater, and various corrosive media such as acids, salts, and alkalis. These U-bends are commonly used in shell-and-tube heat exchangers and feature high tensile strength, excellent weldability, and the ability to withstand high pressures and chemical attack in a variety of industrial applications.
What is UNS N04400?
MONEL Nickel-Copper Alloy 400 (UNS N04400/W.Nr. 2.4360 and 2.4361) is a solid-solution alloy that can only be hardened by cold working. It exhibits high strength and toughness over a wide temperature range and offers excellent corrosion resistance in a wide range of corrosive environments.

Monel Alloy 400 Tube Material Specification Chart
| ASTM B163 Alloy 400 Tubing Standards | ASTM B163/ ASME SB163, ASTM B730/ ASME SB730 UNS 4400 Tubing |
|---|---|
| ASTM B163 Alloy 400 Seamless Tube Size | 3.35 mm OD To 101.6 mm OD |
| ASTM B163 Alloy 400 Welded Tube Size | 6.35 mm OD To 152 mm OD |
| ASTM B730 Monel 400 Tubing Swg & Bwg | 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg. |
| Inconel WERKSTOFF NR. 2.4360 Tube wall thickness | 0.020" –0.220", (special wall thicknesses available) |
| Monel UNS N04400 Tubing Length | Single Random, Double Random, Standard & Cut length Tube |
| Inconel WERKSTOFF NR. 2.4360 Tubing Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| Form | 'U' bent, Hollow, Hydraulic, LSAW, Boiler, Straight Tube, Tube Coil, Round, Rectangular, Square Etc |
| Types of 400 Alloy Tubing | Seamless, ERW, EFW, Welded, Fabricated Tube / Tubing |
| 400 Alloy Tube End | Plain End, Beveled End, Treaded Tube |
| Marking | All ASTM B163 Monel 400 Tubing are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.) |
| Application & uses of Monel 400 Tube | Oil Tube, Gas Tube, Fluid Tube, Boiler Tube, Heat exchanger Tube, |
Monel 400 U-bends refer to a special type of tubing made from Monel 400. Monel 400 is a nickel-copper alloy known for its exceptional corrosion resistance in a variety of environments, including seawater, acidic, and alkaline solutions. The "U-bend" design of these tubings means they are bent into a U-shape, with two straight sections connected by a semicircular bend.
These U-bends are commonly used in heat exchangers, condensers, boilers, and other industrial applications that require a U-shaped structure for a specific purpose. The U-bend design allows for efficient fluid flow and heat transfer within a compact space, making it an ideal choice for space-constrained applications.
Monel 400 offers excellent corrosion resistance in a wide range of environments, making it ideal for applications involving contact with corrosive substances. Its good mechanical properties and high strength provide durability and reliability in demanding applications. These tubings can withstand high temperatures and thermal cycling, making them ideal for heat transfer applications. Monel 400 is easily welded, allowing for the fabrication of complex tubing, such as U-bends. Monel 400 U-Bends are widely used in industries such as chemical processing, marine, oil and gas, aerospace, and power generation where corrosion resistance and high performance are critical.
Alloy 400 Heat Exchanger Tube composition and properties
| Element | Content |
| Ni |
63 % min |
| Cu |
28 - 34 % |
| Fe |
2.5 % max |
| Mn |
2 % max |
Typical Properties of Monel 400 Tube
Typical properties of Monel 400 Tube are covered in the following table.
| Property | Metric | Imperial |
| Density | 8.8 g/cm3 | 0.318lb/in3 |
| Melting point | 1350°C | 2460°F |
| Co-Efficient of Expansion | 13.9µm/m.°C (20-100°C) |
7.7x10-6 in/in.°F (70-212°F) |
| Modulus of rigidity |
65.3 kN/mm2 |
9471 ksi |
| Modulus of elasticity | 105-120 kN/mm2 | 15230-17405 ksi |
Properties of Supplied Materials and Heat Treated Materials
| Condition of Supply | Heat Treatment (After Forming) | |||
| Annealed/Spring Temper | Stress relieve at 300-320°C (570-610°F) for 1 hour and air cool. | |||
| Condition | Approx Tensile Strength | Approx Service Temp. | ||
| Annealed | 400 - 600 N/mm2 | 58 - 87 ksi | -200 to +230°C | -330 to +445°F |
| Spring Temper | 850 - 1050 N/mm2 | 123 - 152 ksi | -200 to +230°C | -330 to +445°F |
Applications
Heat Exchangers: Due to their U-shaped structure and corrosion resistance, they are widely used in shell-and-tube heat exchangers.
Industrial Uses: They are a popular choice for high-pressure and chemically corrosive applications in various industrial sectors.
Shapes and Specifications
U-Bends: Pipes are bent into a U-shape, a common configuration in heat exchanger tube bundles.
Seamless Tubing: ASME SB163 specifies the use of seamless tubing, which is manufactured from a single piece of steel, ensuring superior strength and reliability.
Dimensional Tolerances: Specific dimensional tolerances are applied, especially in the bends of the U-shaped tubes.
Limitations
Oxidizing Acids: Monel 400 is not suitable for use with oxidizing acids, such as nitric acid or nitrous acid.
Sour Gases: It is susceptible to attack by sour gases at temperatures above approximately 700°F (371°C).

Gnee Steel specializes in the production of various nickel-based alloys. Gnee Steel's product packaging includes steel strapping: Pipes with an outer diameter of 3 inches or less are typically strapped together with polypropylene film to prevent rust during sea transportation, and then secured with steel strapping. Wooden boxes/crates: Pipes are typically packaged in wooden boxes or crates to protect them during transportation, especially those that are longer or have larger diameters. Seaworthy export packaging: Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipes during transportation. Tarpaulin packaging: This prevents rain, seawater, and other external factors from penetrating the export wooden crates during transportation. Gnee Steel specializes in the production and sale of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions based on customer needs. For alloy material pricing inquiries or customized alloy material solutions, please contact us for a quote at ss@gneesteel.com.