Advantages of stainless steel pipe fittings and welding precautions
Stainless steel pipe fittings are a widely used pipe fitting product. In order to meet the needs of the majority of users, products such as stainless steel elbows, stainless steel tees, etc. are derived. These are collectively referred to as stainless steel pipe fittings and are deeply loved and favored by people in the industry. Below, GNEE Steel will take you through the advantages and welding precautions of stainless steel pipe fittings.


Advantages of ss pipe fittings:
1. It has good corrosion resistance and oxidation resistance.
2. The coatings of stainless pipe fittings are divided into two types, one is titanium calcium type and the other is low hydrogen type. The former one can be used for AC and DC, and can turn red quickly during welding.
3. The welding rod should be continuously dried during operation. The titanium-calcium type drying should be controlled at 150 degrees Celsius for 1 hour; the low hydrogen type should be controlled at 200~250 degrees for 1 hour. When drying, you cannot dry it once, otherwise the drug skin will crack.
4. Stainless steel pipe fittings also have heat resistance and wear resistance, so they are used in chemical industry, power stations, petroleum and other equipment.
Precautions for welding stainless steel pipe fittings:
1. When welding stainless steel pipe fittings, heat treatment will precipitate carbides, reducing corrosion resistance and mechanical properties.
2. The welding current should not be too long, and the arc should not be too long. Narrow welding seams should be the dominant method.
3. Stainless steel pipe fittings are prone to cracks during welding, so welding requires heat treatment.
4. There should be no dirt on the surface of the welding rod coating to avoid quality problems.