About Incoloy 800H Copper-Nickel Alloy SMLS Boiler Tubes
Incoloy 800H alloy tubing is an iron-nickel-chromium alloy, not a copper-nickel alloy, designed for high-temperature and corrosive environments. Its primary advantages are high strength and resistance to oxidation, carburization, and sulfidation in high-temperature applications such as power plants and petrochemical plants. The term "copper-nickel alloy" in your query is incorrect; Incoloy 800H tubing is a nickel-based alloy. Its seamless (SMLS) boiler tubes are suitable for demanding applications where other materials may fail.
What is the difference between Incoloy 600 and Incoloy 800?
Incoloy 800 has a higher iron content. Its higher iron content and lower nickel content result in a lower cost. Furthermore, due to its affordability, Inconel 600 is considered an ideal material for high-temperature applications.

Specification Of 800 Incoloy Copper-Nickel Alloy SMLS Boiler Pipe
| Pipe Standard | ASTM B407, ASTM B514, B515, ASME SB407, SB514, SB515 |
| Type | Seamless & Welded |
| Size Range | 6mm OD to 600 OD |
| Thickness | 1mm to 20mm |
| Schedule | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Value Added Services | Cutting, Beveling, Polishing, Threading, Destructive, Non Destructive, Ultrasonic Testing |
Chemical Composition Of Incoloy 800 High Temperature Pipe
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr | Al | Ti |
| 800H | 0.05 – 0.10 | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60 | 0.15 – 0.60 |
Mechanical Properties Of 800 Incoloy High Temperature Tubing
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1385 °C (2525 °F) | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa – 205 | 30 % |
Key Features
Material: Nickel-iron-chromium alloy, not copper-nickel alloy.
Shape: SMLS (seamless) pipe offers superior strength and pressure-bearing capacity compared to welded pipe, making it an ideal choice for high-pressure and corrosive applications.
High-Temperature Strength: Engineered to maintain structural integrity and mechanical properties at elevated temperatures, it outperforms standard stainless steel.
Corrosion Resistance: Excellent resistance to oxidation, carburization, and sulfidation, making it suitable for aggressive chemical and thermal environments.
Creep Resistance: Incoloy 800H's higher carbon content and controlled grain size significantly improve its creep and stress-rupture resistance at elevated temperatures.
Key Applications
Power Generation: Used in coal-fired power plants and other facilities requiring high-temperature resistance.
Petrochemical Industry: Used in refineries and processing plants handling corrosive chemicals and high temperatures.
Heat Treatment: Used in furnaces and heat-treating equipment requiring reliable performance at extremely high temperatures.
Chemical Processing:
Suitable for applications involving corrosive compounds and distillation processes.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.