A Comprehensive Guide To Nickel-Based Superalloys: Incoloy 800H (UNS N08810/W.Nr. 1.4958)

A Comprehensive Guide to Nickel-Based Superalloys: Incoloy 800H (UNS N08810/W.Nr. 1.4958)

 

 

What is Incoloy 800H?

Incoloy 800H, also known as "Alloy 800H", is designated UNS N08810 or DIN W.Nr. 1.4958. Its chemical composition is almost identical to Incoloy 800 except that it requires a higher carbon addition, which improves high temperature properties. It has better creep and stress rupture properties than Incoloy 800 in the temperature range of 1100°F [592°C] to 1800°F [980°C]. Incoloy 800 is usually annealed at about 1800°F [980°C], while Incoloy 800H should be annealed at about 2100°F [1150°C]. In addition, according to ASTM 800, alloy 5H has a coarser average grain size.

A Comprehensive Guide to Nickel-Based Superalloys: Incoloy 800H (UNS N08810/W.Nr. 1.4958)A Comprehensive Guide to Nickel-Based Superalloys: Incoloy 800H (UNS N08810/W.Nr. 1.4958)

Incoloy 800H (UNS NO8810) Nickel-based high-temperature alloys usually contain n 15-25% chromium. The nickel content is 30-45%, and contains a small amount of aluminum and titanium. Compared with Incoloy 800 alloy, the carbon content is controlled from ≤0.1% to 0.05-0.1%, which better improves the strength of the steel. The alloy has a high chromium content and sufficient nickel content, so it has high high-temperature corrosion resistance and is widely used in industry. In chlorides, low-concentration NaOH aqueous solutions and high-temperature and high-pressure water, it has excellent resistance to stress corrosion cracking, so it is used to manufacture stress corrosion cracking resistant equipment. The corrosion resistance is better than that of general austenitic stainless steel and Inconel 600 alloy; in the manufacture of corrosion-resistant stress cracking equipment, it is better than Inconel 600 and Monel 400.

Application fields Nickel-based alloy Heat-resistant nickel-iron alloy 800h (N08810)

Chemical industry
Nuclear generator
Nitric acid cooler
Acetic anhydride cracking tube
Heat exchange equipment
Heat exchange tube
Fittings
Flange
Valve

Heat treatment of Nickel-based alloy Heat-resistant nickel-iron alloy 800h (UNS N08810)

(1) Temperature range 1200℃-950℃, cooling method is water quenching or rapid air cooling.
(2) In order to obtain the best performance and creep resistance, solid solution treatment should be carried out after hot working.
(3) The material can be directly sent into a furnace heated to 1200℃. After sufficient insulation time, it can be quickly discharged and heat treated within the specified temperature range. When the material temperature drops below the heat treatment temperature, it needs to be reheated.
Cold working of Incoloy 800H (NO8810) alloy
(1) The work hardening rate is greater than that of austenitic stainless steel, so the processing equipment needs to be selected. The cold-worked material should be in a solution heat treatment state, and intermediate annealing should be performed when the cold working amount is large.
(2) If the cold working amount is greater than 10%, the workpiece needs to be subjected to secondary solution treatment.
Welding process of nickel-based alloys Heat-resistant nickel-iron alloy 800h (UNS N08810)
Suitable for welding with the same material or other metals using any conventional welding process, such as tungsten inert gas shielded welding, plasma arc welding, manual sub-arc welding, metal inert gas shielded welding, MIG welding, and pulse arc welding are the first choice. If manual arc welding is used, it is recommended to use (Ar+He+H2+CO2) as the shielding gas.