Monel R-405 Plate
video

Monel R-405 Plate

Monel R405 is the free machining version of Monel 400. It is a nickel-copper alloy with a controlled amount of sulfur added to provide sulfide inclusions that act as chip breakers during machining.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel r-405 plate in China. If you're going to wholesale high quality monel r-405 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel R-405 Plate

Product Introduction

Monel® R405 is a solid solution nickel-copper alloy that can only be hardened by cold work. It is slightly magnetic at room temperature. It is the free-machining grade of Monel 400. The sulfur content in the element is increased and the workability is improved. It maintains the corrosion resistance, high strength and good weldability of Monel 400, but the mechanical properties are slightly different, and it is mainly recommended for screw machines.

Specification Of Monel R-405

Chemical Composition
C Mn Fe Ni Cu Si S
0.3 Max 2.0 Max 2.5 Max 63.0 Min 28.0 - 34.0 0.5 Max 0.025-0.060
Mechanical Properties
Condition Tensile (ksi) Yield (ksi) Elongation % Hardness Brinell (3000 kg) Hardness Rockwell B
Annealed 70-85 25-40 50-35 110-140 60-76
Hot-Finished 75-90 35-60 45-30 130-170 72-86
Cold-Drawn, As-Drawn 85-115 50-105 35-15 160-245 85-23C

monel material

Features Of Monel Alloy R-405

● Good machinability, recommended for automatic screw machines

● Resistant to high temperature sea water and steam

● Resistant to corrosion by fast flowing brackish water and sea water

● Can resist stress corrosion cracking in fresh water

● After degassing, it is resistant to hydrofluoric acid and hydrochloric acid

● Good corrosion resistance in neutral and alkaline salts

● Outstanding mechanical performance in a wide temperature range (including sub-zero temperature)

● Excellent resistance to chloride ion stress corrosion cracking

Applications Of Monel Alloy R-405

Monel R-405 is mainly used for valve parts and fasteners for corrosive marine and seawater applications, and blanks for automatic screw machines. It is generally not recommended for other applications.

Hot Tags: monel r-405 plate, China monel r-405 plate suppliers, alloy payment, chemical industry alloy, alloy loss, machining tolerance alloy, alloy return on investment, alloy contract