Monel 405 Alloy Bar
video

Monel 405 Alloy Bar

Monel 450 or Alloy 450, houses a 70-30 combination of copper and nickel, respectively. This variant of the Monel alloy family comes with superior weldability. The alloy possesses fair resistance to bio-fouling or corrosion in the seawater.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 405 alloy bar in China. If you're going to wholesale high quality monel 405 alloy bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel 405 Alloy Bar

Product Introduction

This Monel R405 alloy is the free machining version of Monel 400. This Monel 400 alloy is a nickel-copper alloy with a regulated amount of sulfur added to it to supply sulfide inclusions that act as chip breakers during machining.
GNEE Steel is one of the best manufacturers, suppliers, and exporters of the Monel R405 Round Bars. We are remembered for our high quality products, made using the greater quality of materials per national and international quality standards. We offer these Round Bars in various types to our regarded customers to assemble their requirements. In addition, we offer these bars in custom-made specifications, including diverse shapes, sizes, classes, types, grades, standards, etc.

EQUIVALENT GRADES MONEL R405 ROUND BARS

STANDARD WERKSTOFF NR. UNS
Monel R405 – N04405

CHEMICAL COMPOSITION OF MONEL R405 ROUND BARS

Grade Fe C Ni Mn Si S Cu Al
Monel R405 2.5 max 0.3 max 63 min 2.0 max 0.5 max 0.025 – 0.060 28.0-34.0 –

MECHANICAL PROPERTIES OF MONEL R405 ROUND BARS

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.8 g/cm3 1300 – 1350°C 550 Mpa 240 Mpa 40%

product-825-184

Benefits of Monel R405 Round Bars:

It is ASME for use in boilers, pressure, and nuclear vessels

It can be fabricated and heat-treated

 

Uses of Monel R405 Round Bars:

These bars are generally used in the following application :

Brine heaters, sea water scrubbers in tanker inert gas systems

Sulfuric and hydrofluoric acid alkylation plants.

Pickling bat heating coils.

Heat exchangers in a variety of industries.

Transfer piping from oil refinery crude columns.

Hot Tags: monel 405 alloy bar, China monel 405 alloy bar suppliers, nickel copper alloy, alloy engineering, hydrogen embrittlement resistant alloy, electrical conductivity alloy, tensile strength alloy, alloy industry reputation