Monel Alloy 450 cold rolled Sheet
video

Monel Alloy 450 cold rolled Sheet

As a leading Monel 450 alloy supplier and manufacturer, Gnee Steel specializes in providing premium quality Monel 450 products that offer extreme corrosion resistance and mechanical reliability. Below is a comprehensive technical guide to this advanced alloy.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy 450 cold rolled sheet in China. If you're going to wholesale high quality monel alloy 450 cold rolled sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel 450 cold rolled Sheet introduce

Alloy 450 cold rolled Sheet

Monel Alloy 450 cold rolled SheetMonel Alloy 450 cold rolled Sheet

Monel 450 or Alloy 450, houses a 70-30 combination of copper and nickel, respectively. This variant of the Monel alloy family comes with superior weldability. The alloy possesses fair resistance to bio-fouling or corrosion in the seawater.

With this alloy, you also get access to high fatigue strength along with optimum thermal conductivity. The Monel 450 is used excessively for the creation of condenser plates, seawater condensers, evaporator tubes, distiller tubes, saltwater piping, as well as tubes for heat exchange.

Monel 450 Product Specifications

​Product Form ​Thickness ​Width ​Length ​Surface Finish
​Sheet 0.2–25 mm 500–2500 mm 1000–6000 mm 2B, BA, Polished, Mill Finish
​Plate 5–100 mm 1000–3000 mm 2000–12000 mm Hot-Rolled, Pickled, Machined
​Coil 0.1–4 mm 200–1500 mm Custom Cold-Rolled, Annealed

Chemical Composition of Monel 450

​Element ​Ni ​Cu ​Fe ​Mn ​Si ​C ​S
​Weight % 63–67 27–33 ≤2.5 ≤1.5 ≤0.5 ≤0.15 ≤0.01

Mechanical Properties:

Yield Strength (Minimum) Tensile Strength (Minimum) Elongation (Minimum)
KSI MPA KSI MPA Percentage
24 165 56 385 46

Physical Properties:

Density Thermal Conductivity Melting Range Electrical Resistivity
G/CM3 W/M.K °C °F µΩ·m
8.91 29.4 1170 to 1240 2140 to 2260 412

Monel Alloy 450 Sheet 

Monel Alloy 450 cold rolled Sheet

GNEE Group Factory Environment

450 Sheet

Monel Alloy 450 cold rolled Sheet

GNEE Group Product Packaging

Alloy 450 Sheet

Monel Alloy 450 cold rolled Sheet

FAQ

Q:How does Monel 450 compare to Monel 400?

A:Monel 450 offers enhanced thermal stability and slightly higher strength due to optimized alloying elements.

Q: Can Gnee Steel provide thin Monel 450 foil?
A: Yes, we produce foil as thin as 0.05 mm for special electrical applications.

Q:Are your Monel 450 products traceable?

A:All orders include Mill Test Certificates (MTCs) with EN 10204 3.1 certification.

Q:What's the lead time for custom-sized Monel 450 plates?

A:Standard orders ship in 10–20 days; expedited options available upon request.