Dec 03, 2024 Leave a message

What is the material specification of 2.4816?

2.4816 alloy can maintain its initial mechanical properties at high temperatures, has anti-oxidation properties, and has excellent resistance to corrosion and thermal stress.

2.4816 alloy
 Inconel Alloy 600 Chemical composition :
- Nickel (Ni): 72-75%
- Chromium (Cr): 14.0-17.0%
- Iron (Fe): 6.0-10.0%
- Aluminum (Al): ≤0.30%
- Titanium (Ti): ≤0.30%
- Carbon (C): ≤0.10%
- Silicon (Si): ≤0.50%
- Manganese (Mn): ≤1.00%
- Phosphorus (P): ≤0.020%
- Sulfur (S): ≤0.015%
- Copper (Cu): ≤0.30%

 

The physical properties of 2.4816 include:
- Density: about 8.2 g/cm³
- Melting point: about 1350-1400°C
- Thermal conductivity: about 12 at room temperature W/(m·K)
- Linear expansion coefficient: about 13×10⁻⁶/K in the range of 20-1000°C
- Elastic modulus: about 200 GPa
- Poisson's ratio: about 0.3

 

The mechanical properties of Alloy 600 are as follows:
- Yield strength (Rp0.2): about 355 MPa
- Tensile strength (Rm): about 348 MPa
- Elongation: about 13%
- Section shrinkage: about 41%
- Impact toughness value: 51 J/cm²
- Brinell hardness (HBW): 123

 

2.4816 is mainly used for:
- High-temperature components in the aerospace field, such as engine components and hot end components.
- High-temperature reactors and heat exchangers in petrochemicals.
- Fuel cladding and structural parts in the nuclear energy industry.
- Fasteners and seals in high-temperature corrosion-resistant environments.

2.4816  steel pipe

Production Process
The production process of Inconel Alloy 600 includes:
- Melting: using vacuum induction melting or arc furnace melting.
- Hot working: including forging, rolling or extrusion to improve the microstructure of the material.
- Heat treatment: including solution treatment, aging treatment and possible annealing treatment to obtain the required mechanical properties.

Production Process

Send Inquiry

whatsapp

Phone

E-mail

Inquiry