Hastelloy C-276 (also commonly known as Alloy C-276) is a nickel-molybdenum-chromium alloy known for its excellent corrosion resistance, especially resistance to a variety of chemicals in reducing and oxidizing environments. It is widely used in the fields of petroleum, chemical, pharmaceutical and marine engineering.
About the chemical composition of Hastelloy C-276
Nickel (Ni): about 52.0% to 59.0%
Chromium (Cr): about 14.5% to 16.5%
Molybdenum (Mo): about 15.0% to 17.0%
Tungsten (W): up to 3.0%
Iron (Fe): up to 5.0%
Carbon (C): up to 0.010%
Manganese (Mn): up to 1.0%
Silicon (Si): up to 0.08%
Cobalt (Co): up to 1.0%
Vanadium (V): up to 0.35%
Phosphorus (P): up to 0.040%
Sulfur (S): up to 0.030%
Heat Treatment:
Hastelloy® C-276 cannot be hardened by heat treatment.
Hastelloy C276 Available Surface Finishes:
#1 Hot rolled annealed and pickled. For applications that do not require a smooth decorative surface.
#2D Rough surface after cold rolling, annealing and pickling. For deep drawn formed parts and parts that need to retain lubricants during the forming process.
#2 Smooth surface after cold rolling, annealing and pickling. Light rolling with polished rollers after annealing gives it a brighter surface than 2D.
#2 Cold rolled
#2BA Smooth surface after cold rolling and bright annealing. Light rolling with highly polished rollers produces a shiny surface. The 2BA surface can be used for light forming applications where a smooth surface is required for the formed part.