N06600 alloy pipe is a nickel-chromium alloy that was developed and applied very early. It is widely used in various industries because of its corrosion resistance, heat resistance, curing resistance and good processability.
It has good corrosion resistance in fresh water and fluctuating seawater, and may produce corrosion spots in static seawater. It has high corrosion resistance to various alkaline solutions and most organic acids and compounds, is not easy to produce stress corrosion cracks, and can also be connected by resistance welding, fusion welding or brazing. It is suitable for manufacturing low-load anti-oxidation parts below 1100℃.
Inconel 600 has several similar grades,
such as GH600 (China), NC15Fe (France), W.Nr.2.4816, NiCr15Fe (Germany), NA14 (UK), etc.
inconel 600 alloy steel pipe mechanical properties:
Tensile strength: σb≥550Mpa, yield strength σb≥240Mpa: elongation: δ≥30%, hardness≤100 (HRB)
alloy 600 pipe heat treatment:
Insulate at 980-1150℃ for 1-2 hours, and quickly cool in air or water.
UNS N06600 alloy steel What can be replaced?
The material equivalent to N06600 is 316L stainless steel. 316L stainless steel is a molybdenum-containing stainless steel with similar corrosion resistance and mechanical properties to N06600, and can be used as a replacement material.
As a professional supplier of inconel 600 alloy tubes, GNEE has twelve 8-22 inch cold drawing unit production lines and supporting pickling, annealing, and automatic grinding equipment. The production adopts a real-time online process display and tracking system to effectively ensure production time and quality. The annual production capacity is about 20,000 tons.