Jan 02, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

What is the chemical composition of Inconel 600 seamless pipe?

Inconel 600 seamless alloy tube is a heat-resistant alloy material whose main components are nickel and chromium. It has excellent high temperature resistance, corrosion resistance and oxidation resistance, and performs well in high temperature and extreme environments.

Inconel 600 seamless pipe

Equivalent Material Grade Of Inconel Alloy 600 Pipes

Grade UNS No Old British Euronorm GOST Japanese JIS
BS En No AFNOR
Inconel 600 N06600 NA 13 NiCr15Fe 2.4816 NC15FE11M МНЖМц 28-2,5-1,5 NCF 600

 

Alloy 600 Seamless Pipe Chemical Composition

Grade C Mn Si Fe S Cr Cu Ni
Inconel 600 Pipe min. – – – 6.0 – 14.0 – 72.0
max. 0.15 1.0 0.5 10.0 0.015 17.0 0.5 –

 

Inconel 600 Seamless Pipe Sizes In Mm

WT= wall thickness, OD= Outside Diameter, ID= Inside Diameter

Inconel 600 Pipe OD
mm
Pipe WT
mm
in. Sch Kg/m
13.72 1.65 1/4 10S 0.50
13.72 2.24 1/4 40S 0.64
13.72 3.02 1/4 80S 0.81
17.15 1.65 3/8 10S 0.64
17.15 2.31 3/8 40S 0.86
17.15 3.20 3/8 80S 1.12
21.34 2.11 1/2 10S 1.02
21.34 2.77 1/2 40S 1.29
21.34 3.73 1/2 80S 1.65
26.67 2.11 3/4 10S 1.30
26.67 2.87 3/4 40S 1.71
26.67 3.91 3/4 80S 2.23
33.40 2.77 1 10S 2.13
33.40 3.38 1 40S 2.54
33.40 4.55 1 80S 3.29
33.40 6.352) 1 160 4.30
42.16 2.77 1¼ 10S 2.73
42.16 3.56 1¼ 40S 3.44
42.16 4.85 1¼ 80S 4.53
42.16 6.352) 1¼ 160 5.69
48.26 2.77 1½ 10S 3.16
48.26 3.68 1½ 40S 4.11
48.26 5.08 1½ 80S 5.49
60.33 2.77 2 10S 3.99
60.33 3.91 2 40S 5.52
60.33 5.54 2 80S 7.60
60.33 8.742) 2 160 11.29
73.03 3.05 2½ 10S 5.35
73.03 5.16 2½ 40S 8.77
73.03 7.01 2½ 80S 11.59
88.90 3.05 3 10S 6.56
88.90 5.49 3 40S 11.47
88.90 7.62 3 80S 15.51
88.90 11.132) 3 160 21.67
101.60 3.05 3½ 10S 7.53
101.60 5.74 3½ 40S 13.78
101.60 8.08 3½ 80S 18.92
114.30 3.05 4 10S 8.50
114.30 6.02 4 40S 16.32
114.30 8.56 4 80S 22.67
114.30 13.492) 4 160 34.05
141.30 6.55 5 40S 22.10
141.30 9.53 5 80S 31.44
141.30 15.882) 5 160 49.87
168.28 3.4 6 10S 14.04
168.28 7.11 6 40S 28.69
168.28 10.97 6 80S 43.21
168.28 14.27 6 120 54.75
168.28 18.262) 6 160 68.59
219.08 8.18 8 40S 43.20
219.08 12.7 8 80S 65.63
219.08 18.23 8 120 91.30
219.08 23.012) 8 160 112.97

 

Inconel 600 seamless alloy tubes are widely used in oil refining, chemical processing equipment, nuclear power plants, aerospace, engine parts, high temperature furnaces, heat treatment furnaces, power generation equipment, etc. For example, it can be used to manufacture pipelines, heat exchangers and reactors in petrochemical plants because it can resist strong corrosive media such as sulfuric acid, hydrochloric acid, and nitric acid. 

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry