Introduction to Monel 400
Monel 400, designated UNS N04400, is a nickel-copper alloy containing approximately 63 percent nickel minimum and 28 to 34 percent copper, with iron limited to 2.5 percent maximum. It is a solid-solution alloy and can only be hardened by cold working, not by heat treatment. The alloy is known for good corrosion resistance, good weldability, high strength, and excellent mechanical properties at sub-zero temperatures, which together make it a widely used material in marine and chemical service.
Chemical Composition
The standard composition of Monel 400 per the governing ASTM specifications includes nickel 63.0 percent minimum, copper 28.0 to 34.0 percent, iron 2.50 percent maximum, manganese 2.00 percent maximum, carbon 0.30 percent maximum, silicon 0.50 percent maximum, and sulfur 0.024 percent maximum. The high nickel content combined with copper gives the alloy its characteristic resistance to chloride-containing and reducing environments while retaining strength and ductility.
ASTM Specifications and Product Forms
Monel 400 is supplied in a wide range of product forms under the corresponding ASTM specifications: seamless pipe per ASTM B165, welded pipe per ASTM B725, seamless tube per ASTM B163, plate, sheet, and strip per ASTM B127, rod, bar, and wire per ASTM B164, forgings per ASTM B564, and pipe fittings per ASTM B366. Common equivalent designations include Werkstoff Nr. 2.4360, EN NiCu30Fe, AFNOR NU-30M, and JIS NW 4400, which are useful when sourcing internationally.
Corrosion Resistance
Monel 400 exhibits very low corrosion rates in fast-flowing saltwater and seawater, which is unusual among metals, and excellent resistance to stress corrosion cracking in most freshwaters. It also resists a wide range of non-oxidizing chloride solutions, and it withstands hydrochloric and hydrofluoric acids when they are deoxygenated or outgassed. Because of its high copper content, however, the alloy is rapidly attacked by nitric acid and by ammonia systems, and it should not be selected for those media. The alloy is slightly magnetic at room temperature, a characteristic that should be considered in instrument and magnetic-sensitive applications.
Temperature Capability and Mechanical Behavior
Monel 400 retains excellent mechanical properties at sub-zero temperatures, which supports cryogenic service, and it can be used at temperatures up to about 538 °C (1000 °F) depending on the application and stress level, with a melting point of approximately 1300 to 1350 °C (2370 to 2460 °F). In the annealed condition the alloy is relatively soft, so various tempers produced by cold working are used when higher strength is required. Because the alloy is strengthened only by cold working, design should account for the trade-off between strength and ductility in the selected temper.
Typical Applications
Monel 400 is widely used in marine engineering, chemical processing, oil and gas production, and heat exchanger service. Typical components include seawater piping and pumps, propeller shafts, heat exchanger tubes, valve trim, fasteners, pump and valve components, and process vessels handling reducing acids or alkaline solutions. The alloy is also common in the manufacture of tanks and piping for the storage and transport of chlorides and other corrosive media.
FAQ
Q: What is Monel 400 made of?
A: Monel 400 is a nickel-copper alloy with at least 63 percent nickel and 28 to 34 percent copper, plus small amounts of iron, manganese, carbon, silicon, and sulfur.
Q: Can Monel 400 be hardened by heat treatment?
A: No. Monel 400 is a solid-solution alloy and can only be hardened by cold working. Strength levels are selected through the degree of cold work applied.
Q: Is Monel 400 resistant to seawater?
A: Yes. It exhibits very low corrosion in fast-flowing saltwater and seawater and excellent resistance to stress corrosion cracking in most freshwaters, making it a standard marine alloy.
Q: What acids attack Monel 400?
A: Nitric acid and ammonia systems attack the alloy rapidly because of its high copper content. It performs well in deoxygenated hydrochloric and hydrofluoric acids.
Q: What is the UNS number for Monel 400?
A: UNS N04400, with European equivalent Werkstoff Nr. 2.4360 and EN designation NiCu30Fe.
Q: What ASTM specifications cover Monel 400 products?
A: Seamless pipe per ASTM B165, welded pipe per B725, seamless tube per B163, plate, sheet, and strip per B127, rod, bar, and wire per B164, forgings per B564, and fittings per B366.