Mar 24, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

What is the number for Inconel 600?

What is the number for Inconel 600?

 

 

Inconel Alloy 600
Common Trade Names: Inconel 600; Alloy 600; Nickel 600; Nickelvac 600; Ferrochronin 600.

INCONEL Alloy 600 (UNS N06600 W.Nr. 2.4816) is a standard engineering material for applications requiring corrosion and heat resistance. The alloy also has excellent mechanical properties and presents an ideal combination of high strength and good machinability. The versatility of INCONEL Alloy 600 allows it to be used in a wide variety of applications involving temperatures from cryogenics to over 2000°F (1095°C).

What is the number for Inconel 600?What is the number for Inconel 600?

Available Product Forms:
Tube, pipe, sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, and extrusions.

Specifications
Inconel alloy 600 is designated UNS N06600 and Werkstoff No. 2.4816.

Bars, bars, wire, and forgings: ASTM B 166; ASME SB 166; ASTM B 564; ASME SB 564; AMS 5665; AMS 5687; BS 3075NA14; and 3076NA14; DIN 17752; DIN 17753; and DIN 17754; ISO 9723, 9724, and 9725, MIL-DTL-23229, QQ-W-390.

Plate, Sheet and Strip: ASTM B 168; ASME SB 168; ASTM B 906; ASME SB 906, ASME Code Cases 1827 and N-253, AMS 5540, BS 3072NA14 and 3073NA14, DIN 17750, ISO 6208, EN 10095, MIL-DTL-23228.
Pipe and tubing: ASTM B 167; ASME SB 167, ASTM B 163; ASME SB 163, ASTM B 516; ASME SB 516, ASTM B 517; ASME SB 517, ASTM B 751; ASME SB 751, ASTM B 775; ASME SB 775, ASTM B 829; ASME SB 829, ASME Code Case 1827, N-20, N-253 and N-576, SAE/AMS 5580, DIN 17751, ISO 6207, MIL-DTL-23227

Others: ASTM B 366/ASME SB 366, DIN 17742, ISO 4955A, AFNOR NC15Fe

Send Inquiry