What is Inconel 600 tubing?

What is the difference between Inconel 600 alloy and Inconel 601 alloy?
For sustained high temperatures, Inconel 601 alloy performs better. For low strength or stable high temperatures, Inconel 600 alloy is more suitable. Both have good strength, but Inconel 601 alloy is better able to withstand long-term thermal cycles and creep resistance. Inconel 600 alloy has good acid and chloride corrosion resistance.
What is Inconel 600 tubing?
Inconel 600 nickel-based alloy tube is mainly composed of nickel, chromium, iron and other elements, and has excellent high temperature corrosion resistance and oxidation resistance. The alloy tube has satisfactory thermal strength and high plasticity below 700℃, and can maintain stable mechanical properties in high temperature environment.


What are the sizes of Inconel 600 pipes?
Alloy 600 pipes meet ASTM B167, B829 and B517 specifications. Inconel 600 pipes are available in different sizes as per ASTM, ASME and API standards. Inconel 600 seamless pipes are available in diameters ranging from 4 mm to 219 mm, welded and EFW pipes in diameters ranging from 5 mm to 1219.2 mm, and wall thicknesses ranging from 0.5 mm to 20 mm.
What are the uses of Inconel 600 alloy tubes?
Inconel 600 alloy tubes are used in the electronics field to manufacture parts such as cathode ray tube brackets, thyratron grids, tube brackets and springs. The alloy is a standard manufacturing material for nuclear reactors.

What is Inconel 600 tubing?
Chemical Composition of Inconel 600 Pipe:
| Inconel 600 | Ni | Fe | C | Mn | Si | Cu | Cr | S |
|---|---|---|---|---|---|---|---|---|
| 72.0 min | 6.0 - 10.0 | 0.15 max | 1.0 max | 0.5 max | 0.5 max | 14.0 - 17.0 | 0.015 max |
Mechanical & Physical Properties of Inconel 600 Tubes:
| Density | 8.47 g/cm3 |
|---|---|
| Melting Point | 1413 °C (2580 °F) |
| Tensile Strength | Psi – 95,000 , MPa – 655 |
| Yield Strength (0.2%Offset) | Psi – 45,000 , MPa – 310 |
| Elongation | 40 % |
Gnee Steel UNS N06600 Tubing Schedule Chart
| 1/8" IPS(.405"O. D.) | 3 1/2" IPS( 4.000"O. D.) |
|---|---|
| SCH 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/4" IPS(.540"O. D.) | 4" IPS(4.500"O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 3/8" IPS(.675"O. D.) | 5" IPS( 5.563"O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/2" IPS(.840"O. D.) | 6" IPS(6.625"O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 3/4" IPS(1.050"O. D.) | 8 " IPS(8.625"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 1" IPS:(1.315′O. D.) | 10" IPS(10.750"O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 10, 20, 40, 80 (.500), TRUE 80(.500) |
| 1-1/4" IPS(1.660"O. D.) | 12" IPS(12.750"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH 10, 20, 40(.375), TRUE40(.406), SCH80(.500) |
| 1-1/2" IPS(1.900"O. D.) | 14" IPS(14.000"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH10 (.188), SCH40 (.375) |
| 2" IPS(2.375"O. D.) | 16" IPS(16.000"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH10(.188), SCH40(.375) |
| 2 1/2" IPS(2.875"O. D.) | 18" IPS (18.000"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH-40 (.375) |
| 3" IPS( 3.500"O. D.) | |
| SCH 5, 10, 40, 80, 160, XXH |