What grade is Inconel 625 pipe?

 
What grade is Inconel 625 pipe?
 
Learn about ASTM B444 Nickel Alloy Seamless Pipe Encyclopedia
 

What is the ASTM standard for Alloy 625 pipe?

Inconel 625 is a nickel-chromium-molybdenum-niobium alloy material with a primary nickel content of at least 58%. It is also known as Inconel 625 or UNS NO6625 according to ASTM B444 (pipe) or ASTM B443 (sheet and coil).

 

Which grade does 625 alloy pipe belong to?

Typically, cold worked Inconel 625 alloy seamless pipes are supplied in two conditions, Gr. 1 and Gr. 2. ASTM B444 UNS N06625 Gr 1 pipes are supplied in the annealed condition, while Gr. 2 pipes are supplied in the solution annealed condition.

Performance and application of AISI4130 alloy steel
SS310 Stainless Steel An Industrial Strongman Resistant to High Temperature and Corrosion
 

What is the composition of Inconel 625 metal steel pipe?

Inconel 625 alloy pipe contains at least 58% nickel, 20-23% chromium, up to 5% iron, and 8-10% molybdenum

 

What is the roughness of Alloy 625 Tube?

The best surface roughness result for Inconel 625 Tube is 0.3853 µm. With its excellent strength and corrosion resistance, Inconel 625 Tube is a versatile high-temperature alloy used in a wide range of industries, and its reliability is unquestionable.

Main characteristics of nickel-based alloys and their processing significance

What grade is Inconel 625 pipe?

Inconel 625 pipe is usually cold worked as per ASTM B444 standard. Usually, this cold worked Inconel 625 seamless pipe is supplied in two conditions, namely Grade 1 and Grade 2. ASTM B444 UNS N06625 Gr 1 pipe is supplied in the annealed condition while Grade 2 is supplied in the solution annealed condition. Material 2.4856 Alloy 625 pipe also known as UNS N06625 has many excellent properties. The most critical of these is its corrosion resistance. Inconel 625 pipe is considered very suitable for marine applications for several reasons.

 

The main reason is that the alloy is not only able to withstand high stresses in and out of water but also in a wide range of temperatures. Inconel 625 pipe can also withstand highly sour environments. In addition, ASME Sb 444 UNS N06625 Alloy 625 pipe has properties such as high tensile strength, good creep resistance and good weldability, which makes it useful for nuclear based applications. Inconel 625 welded pipe is a solution strengthened high temperature alloy used in high temperature and high pressure applications. Pipes produced to ASTM B444 UNS N06625 specifications generally indicate that these pipes have seamless construction.

 

Understanding the Difference Between 625 Alloy Grade 1 and 2


625 Alloy Grade 1 is solution annealed and provides excellent resistance to oxidation and corrosion in a wide range of environments. It is widely used in applications that require flexibility, strength, and corrosion resistance at elevated temperatures up to 1100°F (about 577°C).

In contrast, 625 Alloy Grade 2 is solution annealed at elevated temperatures to enhance creep and stress rupture resistance, making it suitable for high-pressure, high-stress applications where durability is critical. The key differences between the two grades are as follows:

Heat Treatment:
Grade 1 steel is typically annealed in the 1600°F to 1800°F (approximately 871°C to 982°C) range to provide good ductility and corrosion resistance while maintaining higher strength than Grade 2 steel.
Grade 2 steel is heat treated above 2000°F (approximately 1093°C) to enhance creep and stress rupture resistance while maintaining corrosion resistance.

Mechanical Properties:Per ASTM B444, ASME SB444, AMS 5581

ConditionTensile StrengthYield StrengthElongation
minimum, ksiminimum, ksiminimum, %
Grade 11206030
Grade 21004030

Applications:
Grade 1 is typically used in marine, oil and gas, aerospace, and chemical processing applications.
Grade 2 is suitable for hydrogen production and hydrogen dissociation catalyst tubes where high temperature performance and corrosion resistance are critical. 

Send Inquiry