Is Alloy 600 Ferromagnetic?

Alloy 600 is normally paramagnetic at room temperature; however, it becomes ferromagnetic at grain boundaries where it is depleted of chromium. This suggests that Alloy 600 can be used for magnetically sensitized nondestructive testing (NDE).

 

What is the difference between Inconel Alloy 600 and Inconel Alloy 601?

Both alloys have good high temperature properties. Among them, Inconel 601 alloy adds more chromium on the basis of Inconel 600 alloy. Therefore, the main difference between them is the difference in oxidation resistance.

Inconel 600 Welded Pipe
Inconel 600 nickel-based alloy seamless pipe
 

What is the difference between Inconel Alloy 800 and Inconel Alloy 600?

Inconel 600 and Incoloy 800 are both high-performance nickel-based alloys, but their main difference is in their composition and therefore their properties. Inconel 600 is a nickel-chromium alloy known for its high strength and corrosion resistance, while Incoloy 800 is a nickel-iron-chromium alloy designed for high-temperature applications. Incoloy 800 generally has a lower nickel content and a higher iron content than Inconel 600.

 

What is the difference between Monel 400 and Alloy 600?

Monel 400 is a nickel-copper alloy. It has excellent corrosion resistance in flowing seawater and is suitable for room temperature corrosion applications. Inconel 600 is a nickel-chromium-iron alloy that is mainly used for high temperature corrosion applications.

Inconel Alloy 600

What is the difference between Inconel Alloy 600 and Inconel Alloy 601?

 

Standard of Inconel 600 & 601

Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet/Plate Bar Forging Fitting Wire
B167 B517 B163 B516 B168 B166 B564 B366 -
B167 B517 B163 - B168 B166 B564 B366 B166

Alloy 600 & 601 Chemical Composition %

Grade Ni Cr Fe C Mn S Si Cu
Inconel 600 72.0 min 14.0 – 17.0 6.0 – 10.0 0.15 max 1.0 max 0.015 max 0.5 max 0.5 max
Grade Ni Cr Al C Mn Si Fe Cu
Inconel 601 58-63 21-25 1-1.7 0.10 max 1.5 max 0.015 max 0.5 max 1.0 max

Inconel 600 & 601 Alloy Mechanical Capacity

UNS Designation Tensile Strength, min Yield Strength (0.2% offset), min Elongation
psi(MPa) psi(MPa) %
N06601 80000 (550) 30000 (205) 30
UNS Designation Tensile Strength, min Yield Strength(0.2% offset), min Elongation
psi(MPa) psi(MPa) %
N06600 80000 (550) 30000 (205) 35

Conclusion
Inconel 601 is superior to Inconel 600 in terms of oxidation resistance. In other aspects, there is not much difference between the two.
Gnee Steel produces high-quality Inconel 600 and Inconel 601 products. If you have any needs, please feel free to contact us. 