Incoloy 800H and 800HT are nickel-iron-chromium alloys that have very good strength and excellent resistance to oxidation and carburization in high temperature environments.
These nickel-steel alloys are indistinguishable except for the large amounts of carbon in the 800H alloy and the expansion of up to 1.20% aluminum and titanium in the 800HT alloy.
Incoloy 800 was the first of these alloys to be changed to Incoloy 800H. This change was made to control the carbon (.05-.10%) and grain size to improve stress rupture properties.
Incoloy 800HT has further adjustments to the consolidation levels of titanium and aluminum (.85-1.20%) to ensure ideal high temperature properties.

Incoloy 800H / 800HT Chemical composition
|
C |
Al |
Si |
S |
Ti |
Cr |
Mn |
Fe |
Ni |
Cu |
|
0.1 max |
0.15 - 0.60 |
1.0 max |
0.015 max |
0.15 - 0.60 |
19.0 - 23.0 |
1.5 max |
39.5 min |
30.0 - 35.0 |
0.75 max |
Incoloy 800H / 800HT Mechanical properties
|
Tensile Strength (ksi) |
0.2% Yield Strength (ksi) |
Elongation% in 2 inches |
|
75 |
30 |
30 |
Incoloy 800H / 800HT Physical properties
|
|
Units |
Temperature in°C |
|
Density |
7.94 g/cm³ |
Room |
|
Specific Heat |
0.11 Kcal/kg.C |
21° |
|
Melting Range |
1357 - 1385 °C |
- |
|
Modulus of Elasticity |
196.5 KN/mm² |
20° |
|
Electrical Resistivity |
98.9 µΩ.cm |
20° |
|
Coefficient of Expansion |
14.4 µm/m °C |
20 - 100° |
|
Thermal Conductivity |
11.5 W/m -°K |
20° |
Incoloy 800H / 800HT Sheet Applications
Used in industrial furnaces, heat treatment equipment, chemical and petrochemical processing, superheaters and reheaters in power plants, pressure vessels, heat exchangers, etc.