Nov 29, 2024 Leave a message

What is the chemical composition of Hastelloy X pipe?

Hastelloy X is a nickel-chromium-iron-molybdenum superalloy. This alloy offers excellent high temperature strength, fabricability, and oxidation resistance. Alloy X has oxidation resistance up to 2200°F. In addition, this nickel steel alloy has been observed to have excellent resistance to stress corrosion cracking in petrochemical applications. The matrix hardness provided by the molybdenum content results in a solid solution alloy with high strength and good fabrication characteristics.

Hastelloy X

Product Specifications

Product Name Hastelloy B-2 Tube
Outside diameter Round tube

4mm-200mm

Square tube

10*10mm-100*100mm

Rectangular tube

10*20mm-50*100mm

Wall thickness

0.6mm-6.0mm

length 1-6 meters, length can be customized
standard

ASTM / AISI / JIS / GB / DIN / EN

surface Black, bright polishing, rough turning, matte surface treatment, NO.4, BA, etc.
Certificate

ISO / SGS / BV

Production Technology Hot Rolled / Cold Rolled

 

Chemical composition

C

Si

P

S

Cr

Mn

Fe

Co

Ni

Mo

W

0.05 - 0.15

1.0 max

0.04

0.03

20.5 - 23.0

1.0 max

17.0 - 20.0

0.5 - 2.5

Remainder

8.0 - 10.0

0.2 - 1.0

 

Mechanical properties

Tensile Strength (ksi)

0.2% Yield Strength (ksi)

Elongation% in 2 inches

95

35

35

 

Physical properties

 

Units

Temperature in°C

Density

8.22 g/cm³

22 °C

Specific Heat

0.116 Kcal/kg.

Room

Melting Range

1260 - 1355 °C

-

Modulus of Elasticity

205 KN/mm²

Room

Electrical Resistivity

118.3 µΩ.cm

22°

Coefficient of Expansion

13.9 µm/m °C

26 - 93°

Thermal Conductivity

9.1 W/m -°K

21°

 

Application Range

Hastelloy X is used in gas turbines, petrochemicals, industrial furnaces, heat treatment equipment, nuclear engineering, jet engine combustion chambers, cabin heaters, turbine exhaust components, etc.