Gnee Steel is a leading manufacturer and high-quality supplier of Nimonic 75/80/90 bars. We are one of the major manufacturers, suppliers, and exporters of Nimonic 75/80/90 round bars. We produce round bars in various thicknesses, shapes, and custom sizes using premium raw materials. Nimonic 75/80/90 is a common austenitic stainless steel alloy composed of copper and nickel. Our staff meticulously designs Nimonic 75/80/90 round bars, strictly adhering to all national and international standards. These precisely sized spherical bars are available at the best prices.
Contact our professionals to recommend alloys suitable for your project
Nimonic 75 / 80 / 90 Alloy Rod & Bars

Nimonic 75 / 80 / 90 Alloy Rod & Bars
Nimonic 75, 80A, and 90 round bars are high-performance nickel-chromium-based superalloy bars, renowned for their excellent high-temperature strength, creep resistance, and oxidation resistance, and widely used in aerospace, gas turbine, and furnace components. These alloys are available from Gnee Steel, a specialized supplier, in round, square, and flat bars, with a variety of specialized solutions: Alloy 75 bars are suitable for medium-temperature oxidation resistance, 80A bars for high-temperature strength, and 90 round bars for maximum stress tolerance.
What is NIMONIC 75 material?
NIMONIC 75 alloy is an 80/20 nickel-chromium alloy with added titanium and carbon. This alloy was originally introduced in the 1940s for the manufacture of turbine blades. It is easy to machine and weld, and possesses good corrosion resistance, mechanical properties, and heat resistance.

Nimonic 75 / 80A / 90 Alloy Bar Detailed Information

Nimonic 75 alloy Bar
Nimonic 75 alloy bars, fortified with carbon and titanium, offer exceptional strength and durability in harsh industrial environments. These bars also exhibit excellent machinability, weldability, and oxidation resistance, and withstand high temperatures. Nimonic bars are renowned for their high performance and low-temperature creep resistance. The 75 alloy demonstrates outstanding corrosion resistance, including resistance to pitting, crevice corrosion, and severe stress corrosion cracking.
Nimonic 80A alloy Bar
Nimonic 80A bars are a non-magnetic steel that cannot be heat-treated for quenching but are commonly used in mining and water filtration, often in conjunction with welded or woven screens. We can also supply Nimonic 80 bars in various sizes, grades, and thicknesses at very reasonable prices to meet individual customer needs.


Nimonic 90 alloy Bar
Nimonic 90 round bars are a precipitation-hardening nickel-chromium-cobalt alloy with high tensile strength and creep strength, and a temperature resistance up to approximately 1700 °F (920 °C). NIMONIC 90 bars also exhibit good resistance to high-temperature corrosion and oxidation. NIMONIC 90 alloy bars are widely used in the manufacture of gas turbine blades and discs, hot-working tools, and springs.
1. Nimonic 75 / 80A / 90 Round Bar Specification
|
Standard |
ASTM A276 / ASME SA276 |
|
Round Bar Size |
3mm~ 800mm |
|
Square Bar Size |
4mm* 4mm ~100mm* 100mm |
|
Flat Bar Size |
2mm ~ 100mm |
|
Angle Size |
3mm* 20mm* 20mm~ 12mm* 100mm* 100mm |
|
Thickness |
50 mm to 6000 mm Long |
|
Length |
1 To 6 Meters, Custom Cut Length |
|
Form |
Round, Square, Hex(A/F), Rectangle, Billet, Ingot, Forging Etc |
2. Nimonic 75 / 80 / 90 Bar / Rods Chemical Properties :
|
Grade |
C |
Ni |
Cu |
Cr |
Ti |
Fe |
Mn |
|
|
Nimonic Alloy 75 |
0.08 / 0.15 |
Bal |
0.5 max |
18.9 – 21.0 |
0.2 / 0.6 |
5.0 max |
1.0 max |
|
|
Nimonic Alloy 80A |
0.10 max |
Bal |
0.2 max |
18.0-21.0 |
1.8-2.7 |
3.0 max |
1.0 max |
|
|
Nimonic Alloy 90 |
0.2 max |
18 – 21 |
15 – 21 |
2 – 3 |
1 – 2 |
1.0 max |
0.2 max |
1.0 max |
3. Nimonic 75 Alloy Bars Mechanical Properties
|
Density |
Modulus of Elasticity |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.37 g/cm3 |
GPa – 206 |
MPa – 750 |
MPa – 275 |
42 % |
4. Nimonic 80A Alloy Rods Mechanical Properties
|
Properties |
Tensile strength(annealed) |
Yield Strength (0.2%Offset) |
Elongation |
|
Metric |
1250 MPa |
780 MPa |
30% |
|
Imperial |
181 ksi |
113 ksi |
30% |
5. Nimonic 90 Bars Mechanical Properties
|
Density |
Melting Point |
Coefficient of Expansion |
Modulus of Rigidity |
Modulus of Elasticity (Annealed + Aged) (Spring Temper + Aged) |
|
8.18g/cm³ |
1370°C |
12.7 μm/m °C (20 – 100°C) |
82.5 kN/mm² |
213 kN/mm² 227 / 240 kN/mm² |
Click to download the Nimonic 75 alloy PDF file now
6. Key Characteristics and Differences of Nimonic 75/80A/90 Alloy Bars
Nimonic 75 (UNS N06075) Bar: An 80/20 nickel-chromium alloy with excellent machinability and high-temperature oxidation resistance. Ideal for plate processing and medium-stress heat treatment equipment.
Nimonic 80A (UNS N07080) Round Bar: A precipitation-hardening alloy (nickel-chromium-titanium-aluminum alloy) with excellent creep strength and corrosion resistance, operating at temperatures up to 815°C.
Nimonic 90 (UNS N07090) Round Bar: High cobalt content (15-21%) provides the highest strength and durability, ideal for critical gas turbine components and springs operating at temperatures up to 950°C.]
7. Applications of Nimonic 75/80A/90 Alloy Rods
Aerospace: Jet engine turbine blades, exhaust systems.
Industry: High-temperature furnace components, burner nozzles.
Energy: Gas turbines, power generation components.




8. Gnee Steel Nimonic 75 Alloy Product Forms
Nimonic 75 alloy is supplied in various forms, including:
Round bars/rods
Square bars
Hexagonal bars



Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners

Gnee Steel GH3030 Certificate
📦 Packaging and Shipping
All Nickel Based Alloy products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express
Contact us for the latest export price quote for GH3030 Alloy
FAQ
Q:What is NIMONIC 75 material?
A: The NIMONIC alloy 75 is an 80/20 nickel-chromium alloy containing titanium and carbon as additives. This alloy was first introduced for use as turbine blades during the 1940s. It is readily fabricated and welded. This alloy exhibits good corrosion resistance, mechanical properties and heat resistance.
Q:What is the difference between NIMONIC 80A and NIMONIC 90?
A: Nimonic 80A (N 80A) is nickel–chromium superalloy, strengthened by additions of titanium, aluminum and carbon, developed for application at temperatures up to 1088 K. Nimonic 90 (N 90) is a creep-resistant alloy, developed for application at temperatures up to 1193 K.
Q:What is equivalent to NIMONIC 75?
A:Other designations that are equivalent to nimonic 75 alloy include the following: DIN 2.4630.DIN 2.4951.
Q:What is the composition of NIMONIC 80?
A: Nimonic 80/80A alloys are primarily composed of nickel and chromium and they are well-known for their high-temperature, low-creep and high performance. That's why UNS N07080 Nimonic 80/80A are called as super alloys. Additives like aluminum, carbon and titanium are infused into the alloy to get the desired properties.