Comparison of Nimonic 75 and 80A high-performance seamless tubing

At Gnee Steel, we are dedicated to bridging the gap between high-performance superalloy materials and the demands of complex industrial infrastructure. As a leading manufacturer and global stocker of high-temperature alloys, Gnee Steel supplies a full range of seamless and welded Nimonic 75 (GH3030) and Nimonic 80A (GH4080A) tubing.

 

Whether you are designing for the extreme high-temperature environments of aerospace combustion chambers or the high-pressure environments of power plants, our tubing solutions provide the reliability and traceability your projects require.

💰 Get a wholesale quote for Nimonic 75 pipes

 
 
 
Comparison of Nimonic 75 and 80A high-performance seamless tubing
Comparison of Nimonic 75 and 80A high-performance seamless tubing
01.

Comparison of Nimonic 75 and 80A high-performance seamless tubing

Nimonic 75 and 80A are both high-performance nickel-chromium-based superalloys used for high-temperature tubing, but they meet different engineering requirements. Nimonic 80A seamless tubing is designed to achieve maximum strength and creep resistance under high loads, while Nimonic 75 high-temperature tubing is more suitable for applications requiring moderate strength, excellent corrosion resistance, good formability, and lower cost.

02.

What is NIMONIC 75 material?

NIMONIC 75 alloy is an 80/20 nickel-chromium alloy with added titanium and carbon. This alloy was originally introduced in the 1940s for the manufacture of turbine blades. It is easy to machine and weld, and possesses good corrosion resistance, mechanical properties, and heat resistance.

NIMONIC 75 Material

1. Nimonic 75 vs. Nimonic 80A Tubing Comparison

Understanding the specific advantages of these two alloys is crucial for achieving cost-effectiveness. Our engineering team will assist you in selecting the appropriate grade based on your thermal and mechanical loads.

Nimonic 75 (Alloy 75 / GH3030): The industry-leading choice with superior oxidation resistance. This titanium-stabilized alloy offers excellent ductility, making it ideal for furnace and radiant tube manufacturing.

Nimonic 80A (Alloy 80A / GH4080A): A precipitation-hardening alloy designed for high-stress environments. It exhibits excellent tensile strength and creep rupture strength at temperatures up to 815°C, making it ideal for high-pressure gas manifolds and exhaust valves.

Contact our professionals to recommend alloys suitable for your project

 

2. Specification of Nimonic 75 / 80A Tubes

Parameter Details
Seamless Tube Size 1/2" NB – 16" NB
Outside Diameter 6.00 mm OD up to 914.4 mm OD. Sizes up to 24" NB available Ex-stock. OD Size Steel Tubes available Ex-stock.
Welded Tube Size 1/2" NB – 24" NB
Manufacturing Shapes Round
Schedule Thickness Range SCH 5, SCH 10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Tubes End Types Plain End, Beveled End, Threaded One End, TBE (Threaded Both Ends)
Manufacturing Techniques Seamless / Welded / ERW
Value Added Services Cutting, Beveling, Threading, Destructive, Non Destructive, Ultrasonic Testing

 

3. Equivalent Grades Nimonic 75 / 80A Tubes

STANDARD WERKSTOFF NR. UNS
Nimonic 75 2.4951 / 2.4630 N06075
Nimonic 80A 2.4952 N07080

 

4. Chemical Composition of Nimonic 75 / 80A Tubes

Grade C Mn Si Cu Fe Ni Cr Ti
Nimonic 75 0.08-0.15 1.0 max 1.0 max 0.5 max 5.0 max Bal 18.0-21.0 0.2-0.6
Nimonic 80A 0.1 max 1.0 max 1.0 max 0.2 max 3.0 max Bal 18.0-21.0 –

 

5. Mechanical Properties of Nimonic 75 / 80A Tubes

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.37g/cm3 1340 – 1380 Psi – 104,000 Psi – 40,000 42 %

Click to download the GH3030 alloy PDF file now

 

6. Gnee Steel Nimonic 75 Seamless and Welded Tube Processes

As a full-service manufacturer, Gnee Steel offers a variety of production methods to meet your specific application and budget requirements:

1. Precision Seamless Tubes

Process: Cold drawing and bright annealing.

Advantages: Zero internal defects, highest pressure rating, and aerospace-grade tolerances.

Sizes: Outer diameter 6mm – 219mm; custom wall thickness available.

 

2. High-Performance Welded Tubes

Process: TIG/plasma welding with 100% X-ray inspection.

Advantages: Suitable for large-diameter applications, excellent cost-effectiveness, and uniformity.

Sizes: Outer diameter 10mm – 508mm.

 

Nimonic 75 / 80A Gauge thickness chart

GAUGE THICKNESS RANGE (INCHES) TYPICAL VALUE (INCHES)
22 0.025 through 0.029 0.028
20 0.031 through 0.035 0.035
19 0.038 through 0.042 0.042
18 0.044 through 0.049 0.049
17 0.053 through 0.058 0.058
16 0.060 through 0.065 0.065
15 0.066 through 0.074 0.072
14 0.075 through 0.085 0.083
13 0.087 through 0.097 0.095
12 0.101 through 0.111 0.109
11 0.112 through 0.122 0.12
10 0.126 through 0.136 0.134
9 0.140 through 0.150 0.148
8 0.157 through 0.167 0.165
7 0.175 through 0.185 0.18

 

Nimonic 75 / 80A tube outside diameter

NOMINAL PIPE SIZE OD SCH 5 SCH 10 SCH 40 SCH 80
1/2″ 0.84 0.065 0.083 0.109 0.147
3/4″ 1.05 0.065 0.083 0.113 0.154
1″ 1.315 0.065 0.109 0.133 0.179
1-1/4″ 1.66 0.065 0.109 0.14 0.191
1-1/2″ 1.9 0.065 0.109 0.145 0.2
2″ 2.375 0.083 0.109 0.154 0.218
2-1/2″ 2.875 0.083 0.12 0.203 0.276
3″ 3.5 0.083 0.12 0.216 0.3
3-1/2″ 4 0.083 0.12 0.226 0.318
4″ 4.5 0.083 0.12 0.237 0.337

🛠️ Inquire about custom processing of Nimonic 75 pipes

 

7. Why Choose Gnee Steel?

Choosing Gnee Steel as your nickel-based alloy tubing supplier will give you access to a streamlined and efficient factory-direct supply chain:

✅️Traceability Certification: Every shipment comes with a complete EN 10204 3.1 Material Testing Certificate (MTC).

✅️Short Delivery Time: We maintain a large inventory of nickel-based alloys 75 and 80A, ready to ship worldwide.

✅️Global Logistics: We offer door-to-port or door-to-door shipping services with reinforced, sea-ready packaging.

✅️Technical Support: Direct access to metallurgical engineers for material cross-referencing and selection.

Gnee Steel GH3030 Certificate

Gnee Steel GH3030 Certificate

 

📦 Packaging and Shipping

All Nickel Based Alloy products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 Gnee Steel GH3030 Product Packing

 Gnee Steel GH3030 Product Packing

Contact us for the latest export price quote for GH3030 Alloy

FAQ

Q1: Can Nimonic 75 tubes be welded easily?
A: Yes! Nimonic 75 has excellent weldability using standard TIG or MIG methods. It is a solid-solution alloy, making it significantly easier to join than the precipitation-hardened Nimonic 80A, which requires careful heat treatment.

 

Q2: Do you provide full material certification for every order?
A: Absolutely. As a quality-focused manufacturer, every order is accompanied by an ISO-certified MTC detailing the exact chemical composition, mechanical tests, and grain size analysis.

 

Q3: What is the primary benefit of Nimonic 80A over Nimonic 75 for tubing?
A: Nimonic 80A offers much higher creep-rupture strength. If your system must withstand high internal pressure or vibration at temperatures above 700°C, 80A is the safer and more durable choice.

 

Q4: Can you produce non-standard pipe dimensions?
A: We specialize in custom fabrication. We can produce non-standard wall thicknesses and outer diameters to help you minimize weight and material costs without compromising safety.