Gnee Steel is a leading manufacturer and premium retailer of Nimonic 75/80/90 sheet metal. Our Nimonic 75/80/90 sheet metal is widely recognized in the industry for its superior corrosion resistance. Gnee Steel's Nimonic 75/80/90 sheet metal is of exceptional quality, and we consistently use the highest quality raw materials in our production. Nimonic 75/80/90 sheet metal offers excellent corrosion and oxidation resistance, making it suitable for a wide range of applications.
Contact our professionals to recommend alloys suitable for your project
Nimonic 75 / 80A / 90 Sheet

Nimonic 75 / 80A / 90 Sheet
Nimonic 75, 80A, and 90 plates are high-performance nickel-chromium-based superalloy plates, known for their excellent oxidation resistance, creep strength, and high-temperature corrosion resistance, and are commonly used in aerospace, gas turbine, and furnace components.
What is the Nimonic 80A standard?
Nimonic 80A is a nickel-based alloy with excellent heat resistance, good creep resistance, and high-temperature oxidation resistance, with a maximum heat resistance temperature of 815°C. It is produced using vacuum ion melting (VIM) followed by electroslag remelting (ESR) or vacuum arc remelting (VAR) processes to ensure its high degree of cleanliness and homogeneity, thus guaranteeing its superior performance.

1. Specification for Nimonic 75 / 80A / 90 Plates & Sheets :
| Plate Specification | MSRR, AMS, BS, ASTM B463 |
| Length & Sizes | 1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2m, 2.44m, 3m, 36″ X 120″ or 48″ X 144″, Cut to size available |
| Thickness | 0.1mm to 100 mm Thk |
| Width | 10-2500mm |
| AMS | AMS |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
| Temper | Annealed |
| Condition | Polished on both sides |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Stock in form of | Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate |
2. Chemical Composition of Nimonic 75 / 80A / 90 Plates
|
Grade |
C |
Ni |
Cu |
Cr |
Ti |
Fe |
Mn |
|
|
Nimonic Alloy 75 |
0.08 / 0.15 |
Bal |
0.5 max |
18.9 – 21.0 |
0.2 / 0.6 |
5.0 max |
1.0 max |
|
|
Nimonic Alloy 80A |
0.10 max |
Bal |
0.2 max |
18.0-21.0 |
1.8-2.7 |
3.0 max |
1.0 max |
|
|
Nimonic Alloy 90 |
0.2 max |
18 – 21 |
15 – 21 |
2 – 3 |
1 – 2 |
1.0 max |
0.2 max |
1.0 max |
3. Mechanical properties for Nimonic 75 Plates
|
Density |
Modulus of Elasticity |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.37 g/cm3 |
GPa – 206 |
MPa – 750 |
MPa – 275 |
42 % |
4. Nimonic 80A Alloy Sheets Mechanical Properties
|
Properties |
Tensile strength(annealed) |
Yield Strength (0.2%Offset) |
Elongation |
|
Metric |
1250 MPa |
780 MPa |
30% |
|
Imperial |
181 ksi |
113 ksi |
30% |
5. Nimonic 90 Plates Mechanical Properties
|
Density |
Melting Point |
Coefficient of Expansion |
Modulus of Rigidity |
Modulus of Elasticity (Annealed + Aged) (Spring Temper + Aged) |
|
8.18g/cm³ |
1370°C |
12.7 μm/m °C (20 – 100°C) |
82.5 kN/mm² |
213 kN/mm² 227 / 240 kN/mm² |
Click to download the GH3030 alloy PDF file now
6. Nimonic 75 / 80A / 90 Alloy Plate Properties and Applications
Nimonic 75 (UNS N06075) Plate: An 80/20 nickel-chromium alloy with high oxidation resistance, excellent ductility, and moderate strength. Commonly used in plate form for combustion chambers, flame tubes, and heat treatment equipment.



Nimonic 80A (UNS N07080) Alloy Plate: A precipitation-hardening alloy (with added titanium/aluminum), renowned for its tensile strength up to 800°C and creep rupture resistance. Commonly used in turbine blades, fasteners, and exhaust valves.



Nimonic 90 (UNS N07090) Plate: A nickel-chromium-cobalt alloy with higher high-temperature strength and creep resistance than 80A. Used in heavy-duty applications such as discs and blades in gas turbines.



7. Key Characteristics and Machining of Nimonic 75/80A/90 Alloy Sheets
Machining: Easy to machine and weld; annealing is recommended before welding.
Heat Treatment:
Nimonic 75 Sheets: Typically annealed at 1051°C (1925°F) and air-cooled.
Nimonic 90 Alloy Sheets: Typically treated with 8 hours/1080°C/air cooling + 16 hours/700°C/air cooling to obtain optimal microstructure.
Machining Performance: Generally, these high-temperature alloys are difficult to machine due to their high strength at high temperatures; a sharp cutting edge is required.
Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners

Gnee Steel GH3030 Certificate
📦 Packaging and Shipping
All Nickel Based Alloy products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express
Contact us for the latest export price quote for GH3030 Alloy
FAQ
Q1: Can I replace Nimonic 75 with Nimonic 80A in my furnace project?
A: While Nimonic 80A is stronger, it is more expensive and harder to weld. If your project doesn't require high creep strength, staying with Nimonic 75 is more cost-effective.
Q2: Which alloy has the best weldability?
A: Nimonic 75 is the easiest to weld due to its solid-solution structure. Nimonic 80A and 90 require strict pre-heat and post-weld heat treatments (PWHT) to prevent cracking.
Q3: Do you provide equivalents for GH3030, GH4080A, and GH4090?
A: Yes! We manufacture all three alloys to international standards (ASTM, BS, DIN) and can certify them as GH3030, GH4080A, and GH4090 for the Asian and international markets.
Q4: What is the typical lead time for these Nimonic alloys?
A: For stocked bars and sheets, we ship within 7-10 days. For custom forged components or precision tubes, lead times are generally 4-6 weeks.