Inconel Alloy 718 Mechanical Properties and Supply Status

Inconel 718 is a high-strength, corrosion-resistant nickel-based alloy widely used in high-temperature and high-pressure environments such as aerospace and petrochemicals.

 

Mechanical properties
Inconel 718 has outstanding mechanical properties, especially in high-temperature environments, it can maintain high strength and stability.
Its main performance parameters are as follows:
Yield strength: At room temperature, the yield strength of Inconel718 is about 1030MPa, and it can still maintain a yield strength of about 500MPa at 650°C.
Tensile strength: The tensile strength at room temperature can reach 1400MPa, and at 600°C, the tensile strength can still be maintained above 900MPa.
Ductility: Inconel 718 has good ductility, and the elongation after fracture at room temperature is about 15%, indicating that the alloy still maintains good plasticity at high temperatures.
The creep resistance of Inconel718 is excellent at high temperatures, and its creep rate at 650°C is low, which is suitable for applications that are subjected to high temperature stress for a long time.

 

Supply status
The supply status of Inconel 718 alloy usually includes hot rolling, cold rolling, casting and forging, which are suitable for different processing requirements.
Heat treatment status: Inconel718 is usually supplied with aging treatment (720-740°C) after solution treatment (1050°C). This heat treatment method helps to improve the strength and corrosion resistance of the alloy.
Processing form: Common supply forms include plates, bars, pipes and castings to meet different process requirements.
Surface treatment: The alloy is often pickled or mechanically polished to remove the surface oxide layer and improve its surface quality.

Inconel 718 alloyInconel 718 alloy