GNEE Steel is well-known supplier of ASTM A240 Stainless Steel 446 Plate.We maintain over 1000 ton SS 446 Plates in various shape,sizes & coating which makes us one of the largest stockholder 446 SS Plate in China.We are well known trader of Stainless Steel 446 Plates in China .We producing supplier of stainless steel 446 plate & SS 446 Sheet since 1999.We are ISO 9001:2008 certified manufacturer manufacturer of ASTM A240 Grade 446 plate & now we became Distributor of UNS S44600 Sheet & DIN 1.4762 Stainless Steel Plate. We are largest stockist and exporter of ASTM A240 TP446 Stainless steel Plate in China.We offer 446 stainless steel plate in various sizes at best price.


ASTM A240 Stainless Steel 446 Plate Specifications
| Description |
ASTM A240 / ASME SA240 Stainless Steel Plates, ASTM A240 Hot Rolled Stainless Plates |
| Standard | ASTM, ASME, BS, DIN, EN |
| Material | 310S, 310, 309, 309S, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H, 304, 304L, |
| 302, 301, 201, 202, 403, 405, 409, 409L, 410, 410S, 420, 430, 631, 904L, Duplex, etc | |
| Specification | Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.
Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt. |
| Technique | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Form | Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc. |
| Surface | 2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching |
| Thickness | 0.25-200mm, 0.3mm to 120mm |
| Width | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm |
| Package | Standard Export Seaworthy Package, or as required. |
| Value Added Services | Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc. |
| MTC | Mill Test Certificate, Available as per EN 10204 3.1 |
ASTM A240 SS 446 Metal Plate Chemical Composition
| Element | Content (%) |
|---|---|
| Iron, Fe | 73 |
| Chromium, Cr | 23.0 – 27.0 |
| Manganese, Mn | 1.50 |
| Silicon, Si | 1.0 |
| Nickel, Ni | 0.25 |
| Carbon, C | 0.20 |
| Phosphorous, P | 0.040 |
| Sulfur, S | 0.030 |
ASTM A240 SS 446 Sheet Mechanical Properties
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength | 550 MPa | 79800 psi |
| Yield strength (@strain 0.200%) | 345 MPa | 50000 psi |
| Elastic modulus | 200 GPa | 29000 ksi |
| Poisson's ratio | 0.27-0.30 | 0.27-0.30 |
| Elongation at break | 20% | 20% |
| Hardness, Brinell (estimated from Rockwell B) | 159 | 159 |
| Hardness, Knoop (estimated from Rockwell B) | 173 | 173 |
| Hardness, Rockwell A (estimated from Rockwell B) | 51.1 | 51.1 |
| Hardness, Rockwell B | 83 | 83 |
| Hardness, Vickers (estimated from Rockwell B) | 159 | 159 |
ASTM A240 TP446 Stainless Steel Plate Physical Properties
| Properties | Metric | Imperial |
|---|---|---|
| Density | 7.80 g/cm3 | 0.282 lb/in³ |
446 Stainless Steel Plates In Stock list
| ASTM A240 TP446 Stainless Steel 2B Finish Plate | ASTM A240 TP446 Stainless Steel Cold Rolled Plates |
| ASTM A240 TP446 Stainless Steel 4 Finish Plate | ASTM A240 TP446 Stainless Steel 2D Finish Plate |
| ASTM A240 TP446 Stainless Steel CR Plates | ASTM A240 TP446 Stainless Steel 8 Finish Plate |
| ASTM A240 TP446 Stainless Steel Hot Rolled Plates | Stainless Steel ASTM A240 TP446 HR Plates |
| ASTM A240 TP446 Stainless Steel Plates | ASTM A240 TP446 Stainless Steel Chequered Plate |