Overview of ASTM A240 TP431
ASTM A240 TP431 is a martensitic stainless steel plate grade covered by ASTM A240, the specification for chromium and chromium-nickel stainless steel plate, sheet and strip for pressure vessels and general applications. The grade is also designated UNS S43100 and DIN 1.4057. TP431 combines high hardness and strength in the hardened and tempered condition with good corrosion resistance in mild environments, making it a common choice for shafts, valves, fasteners and wear-resistant components.
Chemical Composition
Per ASTM A240, the nominal composition of 431 stainless steel is: carbon 0.20% max, manganese 1.00% max, silicon 1.00% max, phosphorus 0.04% max, sulfur 0.03% max, chromium 15.00-17.00% and nickel 1.25-2.50%. The chromium content provides corrosion resistance, while nickel improves toughness in the hardened condition. The relatively high carbon level allows hardening by heat treatment, which is the defining feature of the martensitic family.
Physical Properties
Typical physical properties of TP431 plate include a density of about 7800 kg/m³, an elastic modulus of about 200 GPa and a mean coefficient of thermal expansion of about 10.2 µm/m/°C from 0-100°C and 12.1 µm/m/°C from 0-538°C. Thermal conductivity is about 20.2 W/m·K at 100°C, and specific heat is about 460 J/kg·K from 0-100°C. These values support design calculations for thermal expansion, heat transfer and structural stiffness in service.
Mechanical Properties and Heat Treatment
In the annealed condition, 431 plate typically shows a tensile strength of about 862 MPa, a 0.2% proof stress of about 655 MPa, elongation of about 20% in 50 mm and a maximum Brinell hardness of about 285 HB. After hardening and tempering, strength rises significantly; for example, tempering around 204°C produces tensile strength near 1345 MPa with yield near 1055 MPa, while tempering around 593°C gives about 1015 MPa tensile and 770 MPa yield with improved toughness. Because properties vary strongly with tempering temperature, the required tempering condition should be specified on the purchase order together with the applicable standard.
Available Forms, Finishes and Sizes
TP431 is available as hot rolled plate and cold rolled sheet in finishes such as 2B, 2D, BA, No. 1, No. 4, No. 8 and 8K, as well as hairline, sand blast, brush and etching surfaces. Common sizes include cold rolled sheets of 1219 x 2438 mm, 1219 x 3048 mm, 1220 x 2440 mm and 1250 x 2500 mm, and hot rolled plates of 1500 x 2000 mm, 1000 x 3000 mm, 1500 x 4000 mm and 1500 x 6000 mm. Thickness generally ranges from 0.25 mm to 200 mm, widths up to 3500 mm and lengths up to 12000 mm, with custom dimensions available on request. Value-added services include cutting, bending, forging, annealing, pickling, polishing and minor fabrication, and material certificates can be supplied in line with EN 10204 3.1.
Selection Notes
Because 431 is a martensitic grade, it is not intended for applications that require the weldability and formability of austenitic stainless steel. It is best selected where hardness, wear resistance and moderate corrosion resistance are needed, such as pump shafts, valve trim, fasteners and cutlery. If the application demands higher corrosion resistance or fully austenitic behavior, 304 or 316 grades should be considered instead; the choice should be based on the actual service media, temperature and mechanical requirements.
FAQ
Q: What is ASTM A240 TP431?
A: It is a martensitic stainless steel plate grade in ASTM A240, designated UNS S43100 and DIN 1.4057, combining high strength and hardness with moderate corrosion resistance.
Q: What is the chromium content of 431 stainless steel?
A: Chromium is 15.00-17.00% with nickel 1.25-2.50%, per ASTM A240 composition limits.
Q: Can TP431 plate be hardened?
A: Yes, as a martensitic grade it is hardened by heat treatment and tempered to a wide range of strength and toughness combinations.
Q: What finishes are available?
A: Common finishes include 2B, 2D, BA, No. 1, No. 4, No. 8 and 8K, plus hairline, sand blast, brush and etching surfaces.
Q: What is the maximum plate thickness?
A: Plate thickness typically ranges from 0.25 mm to 200 mm, depending on width and production route.
Q: Is TP431 suitable for welding?
A: Martensitic grades are weldable with care, including preheat and post-weld heat treatment; for heavily welded structures austenitic or duplex grades are usually preferred.