Inconel Alloy 783 Tube
video

Inconel Alloy 783 Tube

The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783 / U.S. Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt-iron alloy with aluminum, chromium, and niobium additions. The new alloy is of considerable interest to aircraft gas turbine engine designers and materials engineers for containment and clearance control components such as rings, casings, shrouds and seals for compressors, turbines and exhaust systems.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 783 tube in China. If you're going to wholesale high quality inconel alloy 783 tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 783 tube is manufactured from Inconel Alloy 783, a nickel-based superalloy known for its excellent high-temperature strength and corrosion resistance. This alloy is specifically designed to withstand a range of harsh environmental conditions, including high temperatures and aggressive chemical environments.

Uses of Inconel Alloy 783 Tube:

Chemical Processing: It is widely used in the chemical processing industry, especially in equipment that requires exposure to acids and other corrosive chemicals.

Petroleum Refining: In the petroleum industry, it is used in components that come into contact with hydrocarbons and acids during the refining process.

Power Generation: Inconel Alloy 783 tube is utilized in components of power generation systems, such as boilers and heat exchangers, where high-temperature strength is required.

Nuclear Industry: Due to its excellent resistance to high-temperature corrosion, it is also used in certain applications within the nuclear industry.

Aerospace: The alloy's ability to withstand extreme temperatures makes it suitable for aerospace applications, including jet engines and gas turbines.

Physical Properties

Density g/cm3 7.81
lb/in.3 0.282
Melting Range °F 2437 - 2565
°C 1336 - 1407
Specific Heat (21°C) Btu/lb-°F 0.109
J/kg-°C 455

Mechanical Properties

Test Temperature Yield Strength Tensile Strength Elongation Reduction of Area
°F °C ksi MPa ksi MPa % %
70 21 113.0 779 171.0 1194 24 44
800 427 104.0 717 156.0 1076 25 42
1000 538 99.5 686 150.0 1034 25 46
1200 649 99.0 683 142.0 979 28 39
1300 704 88.0 607 117.0 807 39 64

Inconel Alloy 783 tubeInconel Alloy 783 tubeInconel Alloy 783 tube

Hot Tags: inconel alloy 783 tube, China inconel alloy 783 tube suppliers, alloy tubing, inconel alloy receiver parts, inconel alloy timer parts, inconel alloy injection molding process, inconel alloy ss tubing, inconel alloy printed circuit board parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry