Inconel 600 Nickel Alloy Pipe
video

Inconel 600 Nickel Alloy Pipe

Mechanical Properties – Inconel 600 Tube and Pipe
Tensile Strength: Units – ksi (MPa), minimum
Yield Strength: 0.2 % deflection, Units – ksi (MPa), minimum
Elongation: 2 in, Units: %, minimum
Hardness: Units – HRB

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 nickel alloy pipe in China. If you're going to wholesale high quality inconel 600 nickel alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 600 Nickel Alloy Pipe introduce

Inconel 600 Nickel Alloy Pipe

600 Nickel Alloy PipeInconel 600 Nickel Alloy Pipe

Inconel 600 pipe is a commonly used high-temperature alloy pipe, composed of nickel, chromium, iron and other elements. It has good corrosion resistance, high temperature strength and oxidation resistance. It is widely used in petrochemical, aviation, aerospace and other fields. The following is an introduction to Inconel 600 pipes.
characteristic
Inconel 600 pipe has excellent high-temperature strength and corrosion resistance, and can operate stably for a long time under high temperatures and extreme environments. It has strong antioxidant properties and can be used for a long time at high temperatures without failure. Its antioxidant properties can still maintain good stability at 800°C. In addition, Inconel 600 pipes also have good corrosion resistance and can be used for a long time in harsh environments such as strong acids and alkalis.

application
Inconel 600 pipes are widely used in petrochemical, aviation, aerospace and other fields. In the petrochemical industry, Inconel 600 pipes can be used in the manufacturing of oil refining units, chemical reactors, high-temperature furnaces and other equipment; in the aviation and aerospace fields, Inconel 600 pipes can be used in the manufacturing of high-temperature components such as jet engines, gas turbines, and missile engines.

Chemical Composition

  Nickel Chromium Iron Carbon Manganese Sulfur Silicon Copper

Min

72.0

14.0

6.00

Max

17.0

10.00

0.15

1.00

0.015

0.50

0.50

Physical Composition

Density, lb/in3 . 0.306

Density,Mg/m3

8.47

Melting Range, °F

2470-2575

Melting Range, °C

1354-1413

Specific Heat, Btu/lb-°F

0.106

Specific Heat,J/kg-°C

444

Electrical Resistivity, ohm-circ mil/ft

620

Electrical Resistivity, μΩ-m

1.03

Curie Temperature, °F

-192

Curie Temperature, °C

-124

Permeability at 200 oersted (15.9 kA/m)

1.010

Designations & Standards

Forms ASTM ASME DIN

Pipe and Tube

B 167 B 163 B 516 B 517 B 751 B 775 B 829

SB 163 SB 516 SB 517 SB 751 SB 775 SB 829

17751

Inconel 600 Pipe Specifications
Sizes: 15 NB to 150 NB IN
Types: Seamless / ERW / Welded / Fabricated / LSAW Pipes
Standards: ASME SB-167 ASME SB-829 ASME SB-775 ASME SB-725, UNS N06600 / Werkstoff Nr. 2.4816
Lengths: Single Random, Double Random and Cut Lengths.
Shapes: Round, Square, Rectangular, Hydraulic, etc.
Ends: Plain End, Bevel End, Threaded End.

GNEE Group Factory Environment

Inconel 600 alloy factory

600 seamless tubing

FAQ 

Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: Once the products received by customer were found not comply with the products or contract demands, what will you do?
A: We will compensate the customer for all the loss without any hesitation.

Hot Tags: inconel 600 nickel alloy pipe, China inconel 600 nickel alloy pipe suppliers, 625LCF Inconel ss Steel Pipe, inconel alloy pipe fittings, Inconel UNS N06625 Welded Pipe, seamless piping, 625 Round Bars, inconel tube