Inconel Alloy 686
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 686 in China. If you're going to wholesale high quality inconel alloy 686 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment.
Inconel alloy 686 is a single-phase, austenitic Ni-Cr-Mo-W alloy offering outstanding corrosion-resistance in a range of severe environments. Its high nickel (Ni) and molybdenum (Mo) provide good resistance in reducing conditions, and high chromium (Cr) offers resistance to oxidizing media. Molybdenum (Mo) and tungsten (W) aid resistance to localized corrosion such as pitting. Iron (Fe) is closely controlled to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected zones of welded joints. Resistance to general, pitting and crevice corrosion increases with the alloying (Cr+Mo+W) content, and INCONEL alloy 686 scores higher than competitive materials.
Its matched composition welding products, designated as INCO-WELD filler metals and welding electrode 686 CPT also offer exceptional as-welded resistance to sulfuric or hydrochloric acids, to mixtures of the two, and to crevice or pitting corrosion in hot concentrated acid chloride solutions. These welding products are also used for dissimilar and overmatched welding applications.
Alloy 686 is used for resistance to aggressive media in chemical processing, pollution control, pulp and paper manufacture, and waste management applications.
Common Trade Names:
Alloy 686 /Inconel 686 /Nickel686 /UNS N06686 /W.Nr. 2.4606
Specifications:
ASTM B574 ; ASTM B575 ; ASTM B619 ; ISO 15156-3 (NACE MR0175)
Inconel 686 Characteristic
Inconel 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment.
Inconel 686 Chemical Composition
| % | Ni | Cr | Mo | W | Ti | Fe | C | Mn | S | Si | P |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Min | Balance | 19 | 15 | 3 | 0.02 | – | – | – | – | – | – |
| Max | Balance | 23 | 17 | 4.4 | 0.25 | 1 | 0.01 | 0.75 | 0.02 | 0.08 | 0.04 |
Inconel 686 Physical Properties
| Density | Melting Point | Coefficient of Expansion | Modulus of Elasticity |
|---|---|---|---|
| 8.73 g/cm3 | 1338 – 1380 °C | 11.97 gm/m °C (20 – 100 °C) | 207.0 kN/mm2 |
| 0.315 lb/in3 | 2440 – 2516 °F | 6.650 x 10-6 in/in °F (70 – 212 °F) | 30000 ksi |
Inconel 686 Mechanical Properties
| Condition | Tensile Strength Rm N/mm² | Yield strength R P 0. 2N/mm² | Elongation A5% |
|---|---|---|---|
| Solution | 690 | 380 | 45 |
| Cold Drawing/Hot Rolled | 1115 | 1020 | 23.1 |
Inconel 686 Available Shape
Inconel 686 Size Range
Bars & Rods & Foring Ring /Flanges
Sheet & Plate
Strip & Coil
Welding Wire &Spring wire
Seamless Tube & Welded Pipe




Inconel 686 ApplicationsI
They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: inconel alloy 686, China inconel alloy 686 suppliers, high-temperature alloy, inconel alloy transistor parts, inconel alloy plug parts, inconel alloy reducer fittings, inconel alloy oscillator parts, inconel alloy capacitor parts