Incoloy Alloy 925 Metal Steel Coil
video

Incoloy Alloy 925 Metal Steel Coil

Incoloy 925 Sheets, Plates and Coils Specifications
Specifications: ASTM / ASME SB 168
Dimensions: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 925 metal steel coil in China. If you're going to wholesale high quality incoloy alloy 925 metal steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Metal Alloy 925 Metal Steel Coil introduce

Incoloy 925 Metal Steel Coil

Incoloy Alloy 925 Metal Steel CoilIncoloy Alloy 925 Metal Steel Coil

Incoloy 925 steel coil is designed to meet the needs of industries operating in extreme environments. Its combination of corrosion resistance, high strength and thermal stability makes it a reliable choice for critical applications. Whether it is offshore drilling, chemical processing or power generation, Incoloy 925 steel coil provides unmatched performance and durability.
Incoloy 925 is a nickel-iron-chromium alloy with added molybdenum, copper and titanium. It has excellent corrosion resistance, high strength and good processing properties for demanding applications in harsh environments. Incoloy 925 steel coil is widely used in industries such as oil and gas, chemical processing and offshore engineering.

Product Parameter

Product Name

Incoloy 925 Coil

Product Types

Alloy / Alloy Coil

Materials

Nickel-Iron-Chromium Alloy (Incoloy 925)

Standard

ASTM B805, ASME SB805

Thickness

0.05 mm – 5 mm (Customizable)

Width

10 mm – 1250 mm (Customizable)

Surface Finish

No.1, 2B, BA, No.4, 8K, Mirror Finish, Hairline, or as required

Hardness

Annealed or Hardened Condition

Processing Techniques

Hot Rolled, Cold Rolled

Tensile Strength

930 MPa – 1035 MPa

Yield Strength

650 MPa – 725 MPa

Elongation

25% – 30%

Chemical Composition of Inconel 925 Coils

Grade C Mo Si S Cu Fe Ni Cr Al Ti
Incoloy 925 0.01 max 3 max 0.5 max 0.03 max 1.8 28 44 21 0.3 2.1

Mechanical Properties of Inconel 925 Coils

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.05 g/cm³ 1343 °C (2450 °F) Psi – 175000 , MPa – 1210 Psi – 117000 , MPa – 810

24 %

GNEE Group Factory Environment

Alloy 925 Metal Steel Coil

Incoloy Alloy 925 Metal Steel Coil

GNEE Group Product Packaging

925 Metal Steel Coil

Incoloy Alloy 925 Metal Steel Coil

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.