Uns N07725 N06601 Metal Mirror polished Pipe
Good water corrosion resistance.
High mechanical strength.
Simplified manufacturing and processing.
High metallurgical stability.
High flexural strength.
Easy to connect with conventional welding materials and processes.
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n07725 n06601 metal mirror polished pipe in China. If you're going to wholesale high quality uns n07725 n06601 metal mirror polished pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
inconel Products Application
uns n07725 n06601 Metal ss Pipe video
Inconel 601 Pipe Specifications
| Specifications | ASTM B 167 ASME SB 167 / ASTM B 829 ASME SB 829 / ASTM B 517 ASME SB 517 |
|---|---|
| size | 4 to 219mm W. T.: 0.5 to 20mm |
| size | 5.0 mm – 1219.2 mm |
| size | 5.0 mm – 1219.2 mm |
| Specialized in | Large Diameter Size |
| Schedule | SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| Form | Round, Square, Hollow, Rectangular, Hydraulic, Straight Pipes Etc. |
Specifications
▪ Bars and Wire ASTM B 805, ASME Code Case 2217
▪ Bars and Forgings SMC Spec HA91, ASME Code Case 2217
▪ UNS N07725
▪ FMC Spec M40504
▪ NACE MR-0175/ ISO 15156
▪ Inconel 725
inconel Material Specification
Chemcial Composition
| Element | Inconel 601 |
| Ni | 58.0 – 63.0 |
| C | 0.10 max |
| Mn | 1.0 max |
| Cu | 1.0 max |
| S | 0.015 max |
| Si | 0.5 max |
| Cr | 21.0 – 25.0 |
| Fe | Balance |
Chemical Composition of Inconel 725 Pipe
The composition of the Inconel 725 Pipe is crucial for understanding its properties and performance in various industrial applications.
| Grade | Ni | Cr | Al | C | Mn | S | Mo | Si | Cu |
| Inconel 725 | 55.0 - 59.0 | 19.0 - 22.5 | Max 0.35 | Max 0.03 | Max 0.35 | Max 0.20 | Max 0.010 | Max 0.20 | - |


Alloy725 alloy is a nickel-based alloy material composed of nickel, chromium, molybdenum, iron, titanium, aluminum, zirconium, carbon and other elements. Compared with alloy 718, alloy 725 has increased contents of chromium, molybdenum and titanium in its composition. The addition of these elements can enhance the corrosion resistance and wear resistance of the material. In addition, 725 alloy has good high-temperature strength and fatigue life and can be used in high temperatures and extreme environments.
Inconel 601, an alloy material. Excellent oxidation resistance at high temperatures, good resistance to carbonization, good resistance to oxidation in sulfur-containing atmospheres, good mechanical properties at both room temperature and high temperature, good resistance to stress corrosion cracking due to controlled Due to the carbon content and grain size, 601 has higher creep rupture strength, so it is recommended to use 601 in areas above 500°C.
GNEE Group Factory Environment
Uns N07725 Metal Mirror polished Pipe

Customer Case
customer visit


FAQ
Q: How do you make our business establish a long-term and good relationship?
A: We maintain good quality and competitive prices to ensure that our customers benefit; we respect every customer just like our friends and sincerely do business and make friends with them. No matter where they come from.
Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.
Q: About the product price of uns n07725 n06601 Metal Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: Uns N07725 N06601 Metal Mirror polished Pipe, China Uns N07725 N06601 Metal Mirror polished Pipe suppliers, Inconel Alloy, Inconel Welded Pipe, inconel alloy metal tube, Inconel X 750, inconel alloy demodulator parts, inconel alloy oscillator parts
You Might Also Like
Send Inquiry