Inconel 740H 751 Plate
video

Inconel 740H 751 Plate

Inconel is used in many different industries. One of the most common applications for Inconel is in the aerospace industry, namely in the high-temperature environment found within the jet engine. Fuel nozzles, afterburner rings, and other engine components are commonly made out of Inconel. This is because they perform well in the elevated temperature found during operation. They also resist the risk of corrosion presented by jet fuel and other liquids. Inconel is also often used in rockets and space exploration vessels. Common alloys in the aerospace industry include Inconel 625 and Inconel 718.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 740h 751 plate in China. If you're going to wholesale high quality inconel 740h 751 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 740H 751 Sheet

Product Introduction

Products Description

 

Inconel Alloy Products Application
1. Aerospace Applications

2. Chemical Processing Industry

3. Power Generation
4. Maritime Applications
5. Nuclear Industry

 

Inconel Alloy Material Specification
Property 21 °C 204 °C 316 °C 427 °C 538 °C 649 °C 760 °C 871 °C
Ultimate Tensile Strength /Mpa 992.9 923.9 910.1 910.1 896.3 820.5 537.8 275.8
0.2% Yield Strength /MPa 579.2 455.1 434.4 420.6 420.6 413.7 406.8 268.9
Elongation % 44 45 42.5 45 48 34 59 117
Coefficient of Thermal Expansion µm/m⁰C - 13.1 13.3 13.7 14 14.8 15.3 15.8
Thermal Conductivity /kcal/(hr.m.°C) 8.5 10.7 12.2 13.5 15 16.4 17.9 19.6
Modulus of Elasticity/ MPa 2.07 1.93 1.93 1.86 1.79 1.65 1.59 -

nconel 740H 751