ASTM B704 UNS N06625 Welded Alloy Tube
Type:Nickel Pipe
Powder:Not Powder
Outside Diameter:6.0mm to 1219mm
Thickness:0.5mm to 100mm
Application areas: Automobile, petrochemical, industrial, aerospace, energy
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b704 uns n06625 welded alloy tube in China. If you're going to wholesale high quality astm b704 uns n06625 welded alloy tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM B704 UNS N06625 welded alloy pipe is a high-performance alloy pipe, the main components include nickel, chromium, molybdenum and niobium and other elements, with excellent corrosion resistance and high temperature strength.
UNS N06625 Alloy ERW Pipe is widely used in aerospace, marine engineering, chemical processing, power industry and nuclear reactors.
How to weld ASTM B704 UNS N06625 alloy pipe?
Welding method: Use tungsten inert gas arc welding (GTAW) or argon combined arc welding (GTAW+SMAW).
Heat input control: Use multi-layer and multi-pass welding, the thickness of each layer is not more than 4-5mm, and choose low current and high-speed welding.
Weld pass treatment: Stagger the welding between welds, and remove welding slag and debris before continuing.
ASTM B704 Inconel Alloy 625 Welded Tube
Specifications
| Standards | : | ASTM / ASME |
| Designation | : | ASTM / ASME SB 704 |
| Size | : | 4 to 219mm W. T.: 0.5 to 20mm |
| Length | : | Within 13500mm |
| Type | : | Welded |
| Form | : | Round, Square, Rectangular, Hydraulic Etc. |
Inconel Alloy WERKSTOFF NR. 2.4856 Welded Tubing Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.4 g/cm3 | 1350 °C (2460 °F) | Psi - 75,000 , MPa - 517 | Psi - 1,35,000 , MPa -930 | 42.5 % |
ASTM B704 625 Inconel Welded Tube

Why choosing GNEE
GNEE's annual output is about 15,000 tons. The company has a total of 50 rolling mills and 10 wire drawing machines, including 20 automatic precision rolling mills and 6 precision wire drawing machines. The industrial tube production range is 6.35~762mm outer diameter and 0.71~50.8mm wall thickness; the precision BA/EP tube has a diameter of 6.35~60.3mm and a wall thickness of 0.51~5mm.
please contact us for a quote! ss@gneesteel.com
Latest technology inconel alloy 625 testing

Professional nickel-based alloy steel pipe supplier-GNEE

GNEE PACKAGING AND SHIPPING

FAQ
Q. What are your company's main products ?
A: Our main products are stainless steel , carbon steel , galvanized steel, aluminium products , etc.
Q. How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.
Q.What is the difference between UNS N06625 and UNS N08825?
A.The main difference between the two materials is the nickel content value, Inconel 625 has a minimum nickel content of 58%, while Incoloy 825 ranges from 38% to 46%.
Hot Tags: astm b704 uns n06625 welded alloy tube, China astm b704 uns n06625 welded alloy tube suppliers, 625LCF Inconel ss Steel Pipe, inconel alloy combustion chamber parts, inconel alloy camshaft parts, inconel alloy gasket fittings, Inconel Alloy 706 Pipe, inconel alloy multiplexer parts
You Might Also Like
Send Inquiry