Inconel UNS N06601 603XL Alloy hot processed seamless Pipe
video

Inconel UNS N06601 603XL Alloy hot processed seamless Pipe

601 seamless pipe

Outer diameter: 3-600 mm
Wall thickness: 0.5-30 mm
Length: 0.5-12 m

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel uns n06601 603xl alloy hot processed seamless pipe in China. If you're going to wholesale high quality inconel uns n06601 603xl alloy hot processed seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel UNS N06601 603XL Alloy seamless Pipe introduce

UNS N06601 603XL Alloy hot processed seamless Pipe

Inconel UNS N06601 603XL Alloy hot processed seamless PipeInconel UNS N06601 603XL Alloy hot processed seamless Pipe

Inconel 601 Tube is a nickel-based alloy with a high chromium content and a small amount of aluminum, developed specifically to withstand high temperature oxidizing environments during heat treatment of metals and materials. In the metal and glass sectors, it is one of the most widely used thermowell sheath materials and oxygen injection tubes. 601 alloy is able to form a firmly adherent oxide scale that prevents flaking even under severe temperature cycles. The alloy has high strength at high temperatures and retains its ductility even after long periods of use. 601 alloy has good hot corrosion resistance in oxidizing environments. 601 alloy is not recommended for use in strongly reducing sulfur-containing environments. It is suitable for applications that require high heat resistance and high temperature oxidation and corrosion resistance. It has excellent mechanical properties and is easily processed using conventional methods. It is a nickel-chromium-iron alloy with a wide range of uses.

As a leading Inconel pipe supplier in China, AEETHER manufactures and produces a wide range of Inconel 603XL thick wall pipes.

INCONEL 603XL alloy (patent applied for) is a nickel-chromium alloy with added silicon, molybdenum and rare earth elements. The outstanding feature of INCONEL 603XL alloy is its resistance to high temperature oxidation and nitriding.

Inconel 603XL thick wall pipe is a seamless thick wall Inconel 603XL pipe. Compared with Inconel 603XL seamless pipe, it not only inherits the high temperature and corrosion resistance of Inconel 603XL, but also has better high pressure resistance. Therefore, Inconel 603XL thick wall pipe is often used in high pressure equipment. In the manufacturing process, due to the thick wall thickness, cold rolling and cold drawing processes are no longer applicable, so Inconel 603XL thick wall pipe is made of Inconel 603XL round bar perforated and hot rolled.

Inconel 601 Pipes & Tubes Specification

Specifications ASTM B167, B517, B516 / ASME SB167, SB517, SB516
Dimensions ASTM, ASME and API
Size Range 15"NB – 150"NB
Outer Diameter 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness.
Schedule SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS
Type Seamless / ERW / Welded / Fabricated / LSAW Pipes
Length Single Random, Double Random & Cut Length
Form Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tube

Grade 601 UNS (N06601), DIN (2.4851)

Inconel 603XL pipe specifications
Angle steel: 1mm to 1300mm
Pipe: 1mm to 1300mm, also available on request.
Fitting size: 1/8" to 80" (DN6 - DN2000)
Flange size: DN6 - DN2000
Length: available on request.

Chemical Composition Inconel 601 Pipes and Inconel 601 Tubes:

Inconel 601 Ni Fe C Mn Si Cu Cr S Al
58.0 – 63.0 Balance 0.10 max 1.0 max 0.5 max 1.0 max 21.0 – 25.0 0.015 max 1.0 – 1.7

Mechanical & Physical Properties Inconel 601 Pipes and Inconel 601 Tubes:

Density 8.1 g/cm3
Melting Point 1411 °C (2571 °F)
Tensile Strength Psi – 80,000 , MPa – 550
Yield Strength (0.2%Offset) Psi – 30,000 , MPa – 205
Elongation 30 %

Chemical Composition

The chemical composition of INCONEL alloy 603XL is outlined in the following table.

Element Content (%)
Chromium, Cr 15-23
Molybdenum, Mo 4
Silicon, Si 2
Titanium, Ti 0.5 max
Aluminum, Al 0.5 max
Manganese, Mn 0.3 max
Carbon, C 0.3 max
Rare earths 0.1 max
Nickel. Ni Remainder

GNEE Group Factory Environment

Inconel UNS N06601 Alloy hot processed seamless Pipe

Inconel UNS N06601 603XL Alloy hot processed seamless Pipe

GNEE Group Product Packaging

UNS N06601 603XL Alloy hot processed seamless Pipe

Inconel UNS N06601 603XL Alloy hot processed seamless Pipe

FAQ

Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: How long is your delivery time?
A: Generally it is 2-5 days if the goods are in stock or it will need 7-20 days if the goods need to be customized. 

Hot Tags: Inconel UNS N06601 603XL Alloy hot processed seamless Pipe, China Inconel UNS N06601 603XL Alloy hot processed seamless Pipe suppliers, inconel alloy bearing parts, nickel-based, inconel alloy combustion chamber parts, inconel alloy demodulator parts, Inconel Seamless Pipe, inconel alloy ss tubing