Incoloy Alloy 907 Tube
video

Incoloy Alloy 907 Tube

Alloy 907 (Incoloy alloy 907) is a nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of alloy 903 but alloy 907 has improved notch-rupture properties at elevated temperatures.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 907 tube in China. If you're going to wholesale high quality incoloy alloy 907 tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 907 tube is a high-performance material known for its excellent resistance to corrosion and oxidation at high temperatures. It is widely used in applications requiring both high temperature strength and durability. Here are the details about this material, including its characteristics, applications, and manufacturing processes:

 

Chemical Composition:

 

Elements

Content (%)

Iron, Fe

42

Nickel, Ni

38

Cobalt, Co

13

Niobium, Nb

4.7

Titanium, Ti

1.5

Silicon, Si

0.15

Aluminum, Al

0.03

 

Mechanical Properties:

 

Properties

Metric

Imperial

Tensile strength (precipitation hardened, value at room temperature)

1350 MPa

196000 psi

Yield strength (@ strain 0.200%, precipitation hardened, value at room temperature)

1100 MPa

160000 psi

Poisson's ratio

0.36

0.36

Elongation at break (precipitation hardened)

10%

10%

Reduction of area

36

36

 

 

Incoloy Alloy 907 TubeIncoloy Alloy 907 TubeIncoloy Alloy 907 Tube

 

Hot Tags: incoloy alloy 907 tube, China incoloy alloy 907 tube suppliers, alloy for dies, alloy for strengthening, machining alloy, alloy for painting, alloy for anodizing, alloy for laser sintering baths