Incoloy 908
video

Incoloy 908

INCOLOY® alloy 908 (UNS N09908) is an agehardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue crack growth resistance, good ductility, metallurgical stability and weldability plus sufficient resistance to stress accelerated grain boundary oxygen embrittlement (SAGBO) to permit hot fabrication without cracking.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 908 in China. If you're going to wholesale high quality incoloy 908 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy 908 (UNS N09908) is an agehardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue crack growth resistance, good ductility, metallurgical stability and weldability plus sufficient resistance to stress accelerated grain boundary oxygen embrittlement (SAGBO) to permit hot fabrication without cracking. This cobalt-free, low CTE alloy was designed to meet sheathing material requirements for internally cooled Nb3Sn superconductor magnets to be used in prototype fusion reactors at cryogenic operating temperatures of - 452°F (-269°C/4°K). With low temperature properties it is excellent for cryogenic applications.

Main Standards

ASTM B872

Plate, Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.17
lb/in.3 0.295
Melting Range °F 2482 - 2571
°C 1361 - 1410
Curie Temperature °F 539
°C 282
Specific Heat Btu/lb-°F 0.104
J/kg-°C 439
Thermal Conductivity Btu-in/ft2-h-°F 76.68
W/m-°C 11.05
Young's Modulus (70°F) 103 ksi 23.7
GPa 163.3
Shear Modulus (70°F) 103 ksi 9.37
GPa 64.6
Poisson's Ratio   0.265

Mechanical Properties

Unit Value
Tensile Strength
ksi 170
MPa 1172
Yield Strength (0.2% Offset)
ksi 120
MPa 827
Elongation
% 12

product-720-720product-720-720product-720-720product-720-720

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: incoloy 908, China incoloy 908 suppliers, alloy for grinding wheels, alloy for dies, alloy for agile manufacturing baths, alloy for refurbishment baths, alloy for telecommunications, alloy for springs

Send Inquiry

whatsapp

Phone

E-mail

Inquiry