Incoloy 864
video

Incoloy 864

INCOLOY® alloy 864 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stresscorrosion cracking. INCOLOY alloy 864 is covered by U.S. Patent 5,827,377.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 864 in China. If you're going to wholesale high quality incoloy 864 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy 864 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stresscorrosion cracking. INCOLOY alloy 864 is covered by U.S. Patent 5,827,377.

 

Corrosion Resistance

INCOLOY alloy 864 was first developed as a corrosion-resistant material specifically for automotive exhaust systems. Most of the data presented in the following pages relate to that area of application. However, the alloy's potential for other, non-automotive, applications is of sufficient interest to pursue laboratory test programs in other media. Iso-corrosion charts for INCOLOY alloy 864 in hydrochloric and sulfuric acids are presented at the end of this section.

Main Standards

ASTM A240

Sheet and Strip

ASTM A480

Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.02
lb/in.3 0.290
Melting Range °F 2467 - 2539
°C 1353 - 1393
Permeability at 200 oersted (15.9 kA/m)   1.004
Electrical Resistivity at 70°F (21°C) ohm•circ mil/ft 628
μΩ•m 1.04

Mechanical Properties

Test Temperature Hardness Tensile Strength Yield Strength Elongation Fracture Location
Rb ksi MPa ksi MPa %
70°F (20°C) 82 79.9 550.9 46.1 317.9 17.4 Weld
70°F (20°C) 83 80.4 554.4 45.3 312.3 18.7 Weld
800°F (427°C) N/A 64.5 444.7 31.7 218.6 20.5 Weld
1000°F (538°C) N/A 58.4 402.7 30.9 213.1 16.6 Weld
1200°F (648°C) N/A 58.9 406.1 28.9 199.3 18.4 Weld
1400°F (759°C) N/A 40.9 282.0 26.4 182.0 23.5 Weld
1600°F (871°C) N/A 23.4 161.3 15.9 109.6 55.0 Weld

More +

product-720-720product-720-720product-720-720product-720-720

 

 

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

 

Hot Tags: incoloy 864, China incoloy 864 suppliers, Lncoloy 800H, precision alloy rod, alloy for actuators, lncoloy 800 round bar, alloy for regenerative medicine baths, alloy forgings