MA956 PIPE
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ma956 pipe in China. If you're going to wholesale high quality ma956 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
MA 956 pipe represents a high-performance material designed for extreme environments, particularly in the chemical processing and petrochemical industries.
MA 956 is a type of alloy that is known for its exceptional resistance to corrosion, especially in acidic and caustic environments. This makes it suitable for applications where materials are exposed to harsh chemicals at elevated temperatures. While not as well-known as some other alloys like Inconel or stainless steel, MA 956 fills a niche by providing superior performance in very specific, demanding conditions.
Physical Properties
| Density | g/cm3 | 7.25 | |
|---|---|---|---|
| lb/in.3 | 0.262 | ||
| Melting Range | °F | 2700 | |
| °C | 1480 | ||
| Element | Chemical Composition (%) |
|---|---|
| Carbon | 0.26 |
| Silicon | 0.30 |
| Manganese | 1.25 |
| Phosphorus | 0.030 |
| Sulfur | 0.025 |
| Nickel | 0.10 |
| Chromium | 0.30 |
| Molybdenum | 0.08 |
| Copper | 0.40 |
| Niobium | 0.05 |
| Titanium | 0.05 |
| Vanadium | 0.10 |
| Aluminum | 0.02 |
| Cobalt | 0.10 |
| Tungsten | 0.10 |
| Tin | 0.20 |
| Lead | 0.30 |
| Antimony | 0.01 |
| Boron | 0.005 |
| Zirconium | 0.15 |
| Calcium | 0.008 |
| REM (rare earth metals) | 0.01 |



Hot Tags: ma956 pipe, China ma956 pipe suppliers, alloy for high pressure applications, alloy for cleaning baths, alloy for powder bed fusion baths, alloy for packing materials, alloy for vat photopolymerization baths, alloy for relays