Incoloy 864 Alloy Plates
video

Incoloy 864 Alloy Plates

INCOLOY alloy 864 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stresscorrosion cracking. INCOLOY alloy 864 is covered by U.S. Patent 5,827,377.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 864 alloy plates in China. If you're going to wholesale high quality incoloy 864 alloy plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Corrosion Resistance

INCOLOY alloy 864 was first developed as a corrosion-resistant material specifically for automotive exhaust systems. Most of the data presented in the following pages relate to that area of application. However, the alloy's potential for other, non-automotive, applications is of sufficient interest to pursue laboratory test programs in other media. Iso-corrosion charts for INCOLOY alloy 864 in hydrochloric and sulfuric acids are presented at the end of this section.

 

Physical Properties

Density g/cm3 8.02
lb/in.3 0.290
Melting Range °F 2467 - 2539
°C 1353 - 1393
Permeability at 200 oersted (15.9 kA/m)   1.004
Electrical Resistivity at 70°F (21°C) ohm•circ mil/ft 628
μΩ•m 1.04

 

 

Mechanical Properties

Test Temperature Hardness Tensile Strength Yield Strength Elongation Fracture Location
Rb ksi MPa ksi MPa %
70°F (20°C) 82 79.9 550.9 46.1 317.9 17.4 Weld
70°F (20°C) 83 80.4 554.4 45.3 312.3 18.7 Weld
800°F (427°C) N/A 64.5 444.7 31.7 218.6 20.5 Weld
1000°F (538°C) N/A 58.4 402.7 30.9 213.1 16.6 Weld
1200°F (648°C) N/A 58.9 406.1 28.9 199.3 18.4 Weld
1400°F (759°C) N/A 40.9 282.0 26.4 182.0 23.5 Weld
1600°F (871°C) N/A 23.4 161.3 15.9 109.6 55.0 Weld

 

Customer visit

12

2

FAQ

1.What is your working time?

Monday-Saturday : 8:30AM-18:00PM (Beijing time, GMT+08.00) We have public holiday during May.1-3, Oct.1-7 and Chinese New Year holiday . Pls email us during our holiday if u have any question.

2.Do you provide free samples?

Yes, we can provide a free sample for testing,buyer should bear all the shipping costs.

3.What is your payment terms?

T/T,L/C,D/A,D/P,Western Union,MoneyGram,Paypal

 

Others:https://www.chinastainless-steel.com/nickel-alloy-steel/hastelloy/hastelloy-alloy-s-uns-n06635-plates.html

Hot Tags: incoloy 864 alloy plates, China incoloy 864 alloy plates suppliers, Incoloy Metal Tubing, alloy for hardening, alloy for repair baths, alloy for renewable energy, alloy for adsorption baths, alloy for environmental protection baths