Incoloy 800H 825 SMLS tube
video

Incoloy 800H 825 SMLS tube

Applications of Incoloy 825 800H pipes
- Chemical processing
- Food water, seawater thermal containers
- Pollution control equipment
- Sulfuric acid pipelines and containers
- Oil and gas well pipelines
- Nuclear fuel reprocessing
- Acid production
- Pickling equipment
- Radioactive waste treatment
- Water heaters
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800h 825 smls tube in China. If you're going to wholesale high quality incoloy 800h 825 smls tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

incoloy Products Application

Incoloy steel ss Pipe video

Incoloy 800H Pipe Specification

Specifications : ASTM B407 ASME SB407 / ASTM B514 ASME SB514

Size : 15″NB TO 150″NB IN

Schedule :SCH5, SCH10, SCH40, STD, SCH80, SCH160

Form : Round Pipes & Tubes, Square Pipes & Tubes, Rectangular Pipes & Tubes

Type : Seamless / ERW / EFW / Welded / Fabricated

Length : Single Random, Double Random & Cut Length

End : Plain End, Beveled End, Threaded

Outside Finish : 2B, No.1, No.4, No.8 Mirror Finish

Finish : Annealed and Pickled, Polished, Bright Annealed, Cold Drawn

Standard Specifications of Incoloy 825 Tubes
Thickness 0.3mm – 50 mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Outer Diameter 6.00 mm OD to 914.4 mm OD, up to 24" NB
Type Seamless / ERW / Welded / Fabricated / CDW
Shape Round, Square, Rectangular, Coil, "U" Shape, Coil, Hydraulic
Length Single Random, Double Random and Required Length
Ends Plain, Bevel, Threaded.

incoloy Material Specification

INCOLOY 800H Seamless Pipes and Tubes Chemical Composition, UNS NO8800

The chemical composition of Inconel Alloy 800H is provided in the table below:

Ni Cr Fe C Al Ti Al+Ti
30.0-35.0 19.0-23.0 39.5 min .05-.10 .15-.60 .15-.60 .30-1.20

Chemical Equation of Nickel Alloy 825 Tubing

Grade C Mn Si Fe S Cr Cu Ti
825 min. – – – 22.0 – 19.5 1.5 0.6
max. 0.05 1.0 0.5 – 0.015 23.5 3.0 1.2

Incoloy 800H 825 steel Pipe

 

Incoloy 800H 825 alloy steel Pipe priceIncoloy 800H 825 metal Pipe factory

Incoloy 800H (UNS NO8810) Nickel-based superalloy usually contains n 15-25% chromium. Nickel content is 30-45%, with small amounts of aluminum and titanium. Compared with Incoloy 800 alloy, the carbon content is controlled from ≤0.1% to 0.05-0.1%, which better improves the strength of the steel. This alloy has high chromium content and sufficient nickel content, so it has high high temperature corrosion resistance and is widely used in industry. It has excellent resistance to stress corrosion cracking in chloride, low-concentration NaOH aqueous solutions and high-temperature and high-pressure water, so it is used to manufacture anti-stress corrosion cracking equipment. The corrosion resistance is better than that of general austenitic stainless steel and better than Inconel 600 alloy; in the manufacture of corrosion-resistant stress cracking equipment, it is better than Inconel 600 and Monel alloy 400.
Incoloy825 alloy is a NI-FE-MO-CU corrosion-resistant alloy stabilized with Ti. The alloy has effective resistance to uniform corrosion and localized corrosion, and has good performance, so it is widely used in chemistry, energy, and hydrometallurgy. Application. In addition, the alloy has good toughness and performs well in the atmosphere. However, it should be noted that very shallow pitting corrosion will occur in humid atmosphere. This alloy is also resistant to freshwater corrosion and can be used in flowing seawater under all circumstances. However, Certain spots will appear in still seawater or under polluted conditions, so everyone should pay attention to this when producing products. The corrosion resistance of the alloy is very good in various media, such as sulfuric acid, phosphoric acid, and hydrochloric acid. , nitric acid, sulfurous acid, organic acids and compounds. Alkali metals such as sodium hydroxide, potassium hydroxide and hydrochloric acid solutions.

GNEE Group Factory Environment

Incoloy 825 SMLS tube

Incoloy 800H 825 SMLS tube

Customer Case

customer visit

alloy 800H 825 steel Pipe suppliers

Incoloy 800H 825 material Pipe dealer

FAQ

 

 

 

Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. Or if the goods are not in stock, it is 15-20 days, depending on the quantity.

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: About the product price of Incoloy 800H 825 steel Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: Incoloy 800H 825 SMLS tube, China Incoloy 800H 825 SMLS tube suppliers, alloy for spectroscopy baths, alloy for chlorine resistance, Inconel 825 Round Bar, alloy for total quality management baths, alloy parts, alloy for ductility improvement

Send Inquiry

whatsapp

Phone

E-mail

Inquiry