Incoloy 800 Alloy Forged Bars
Quality InspectionUt, Chemical Composition,SGS
Shape:Round/Sauqre/Flat/Hexagon
Process:Cold Drawn,Cold Rolled,Bright Anneal etc
Surface Require:Mirror Polishing, Hairline Finishing, Sb , No.4
Diameter (Od):Cold Drawn Bar:4.76~120mm(All Sizes Can Be Custom)
Application areas: Petrochemical, energy, industrial
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800 alloy forged bars in China. If you're going to wholesale high quality incoloy 800 alloy forged bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Ni 800 Alloy Forged Bars Description

Incoloy 800 alloy rods are also a family of high temperature alloys produced by Specialty Metals. They are nickel-iron-chromium alloys that are used in applications that require high corrosion resistance and high temperature strength. Incoloy alloys are very similar to Inconel alloys, but their applications differ due to their different composition.
800 alloy rod is a material widely used in the manufacture of equipment that must resist corrosion, high strength, or oxidation, carburization, and other harmful effects of high temperatures. The chromium element in the alloy gives it resistance to oxidation and corrosion. The high nickel content allows it to maintain an austenitic structure, which gives it ductility. The nickel element also helps resist scaling, general corrosion, and stress corrosion cracking. The iron element helps resist internal oxidation.
Incoloy 800 Round Bar Sizes
Standard lengths of 2000 to 6000 mm. Cut to size on request (tolerance +2/-0 mm).
| 5.0 mm | 45.0 mm |
| 6.0 mm | 50.0 mm |
| 7.0 mm | 55.0 mm |
| 8.0 mm | 60.0 mm |
| 9.0 mm | 65.0 mm |
| 10.0 mm | 70.0 mm |
| 12.0 mm | 75.0 mm |
| 16.0 mm | 80.0 mm |
| 20.0 mm | 90.0 mm |
| 25.0 mm | 100.0 mm |
| 30.0 mm | 130.0 mm |
| 35.0 mm | 160.0 mm |
| 40.0 mm | 200.0 mm |
Corrosion Resistant 800 Alloy Bar Specification
Incoloy 800 Bars Equivalent Grade
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Incoloy 800 | 1.4876 | N08800 | NCF 800 | NA 15 | ЭИ670 | Z8NC32-21 | X10NiCrAlTi32-20 |
Incoloy 800 Round Bars Chemical Composition
| Grade | C | Mn | Si | Al | S | Cr | Cu | Ni | Fe |
| Incoloy 800 | 0.10 max | 1.50 max | 1 max | 0.15 – 0.60 | 0.015 max | 19.0-23.0 | 0.75 max | 30.0-35.0 | 39.5 min |
Incoloy Alloy 800 Bright Bar Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1385 °C (2525 °F) | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa – 205 | 30 % |
800 Superalloys Products Display
Incoloy 800 Cold Drawn Forged Bar

Why choosing GNEE
GNEE's main products are nickel-based alloy plates/sheets/coils/strips/tubes/rods, etc., with excellent quality and favorable prices.
GNEE has its own factory, professional processing equipment, various types of surface treatment, plasma cutting, water jet cutting, leveling machine, slicer. Since its establishment, we can also process special sizes for customers because we have complete processing equipment, professional technical workers and engineers.
please contact us in time to get a quote!ss@gneesteel.com
Nickel Iron Chromium 800 Alloy Forged Bars Testing
Alloy 800 Round Bars Testing

Alloy 800 Round Bars factory
Alloy 800 Round Bars Factory

About Gnee Steel

Gnee Steel is a supplier of Incoloy 800 Alloy Forged Bars, including Tubes: Seamless Tubes: Sizes: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded Tubes: Sizes: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate Thickness 0.1 to 100 mm; Plate Width 10-2500 mm, Strips, Alloy Round Bars Sizes: Diameter 3-800 mm;, Flat Bars Sizes: Thickness 2-100 mm; Width: 10-500 mm, Hexagonal Bars Sizes: 2-100 mm;, Wires and Extruded Profiles. We work with steel mills to provide our customers with 625 Alloy that meets or exceeds many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Incoloy 800 Alloy Forged Bars, Tubes, Pipes, Plates, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wire and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com
Hot Tags: incoloy 800 alloy forged bars, China incoloy 800 alloy forged bars suppliers, alloy for green manufacturing baths, alloy for additive manufacturing baths, incoloy material pipe alloy, alloy for lean manufacturing baths, high temperature alloys, incoloy pipe alloy
You Might Also Like
Send Inquiry