27-7MO 832 Alloy Seamless Pipe
video

27-7MO 832 Alloy Seamless Pipe

27-7MO alloy is a super austenitic stainless steel containing 7% molybdenum. Compared with 6% molybdenum super austenitic stainless steel,
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 27-7mo 832 alloy seamless pipe in China. If you're going to wholesale high quality 27-7mo 832 alloy seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

27-7MO 832 Alloy Seamless Pipe information

27-7MO 832 Alloy Seamless Pipe video

GNEE STEEL GROUP supplies 27-7MO 832 Alloy Seamless Pipe for you

 

GNEE STEEL GROUP supplies 27-7MO Alloy Seamless Pipe:

Form

Standard

Metal Type

UNS S31277

Bar

ASTM A 479/ASME SA 479

Wire

ASTM A 479/ASME SA 479

Sheet

ASTM A 240/ASME SA 240

Plate

ASTM A 240/ASME SA 240

Tube

ASTM A 213/ASME SA 213 (Tube), ASTM A 249/ASME SA 249

Pipe

ASTM A 312/ASME SA 312

Fitting

ASTM A182

Forging

ASTM A 479/ASME SA 479, ASTM A182

Weld Wire

Weld Electrode

ASME CODE

Allowable design stresses for ASME Boiler and Pressure
Vessel Code construction are defined in ASME Code Case 2458.

Din

GNEE STEEL GROUP supplies 832 Alloy Seamless Pipe:

GNEE STEEL offers Incoloy 832 in various forms including:

Seamless and welded tubes

Seamless and welded tubes

Bars

Wires

Sheets

Forgings

Tube fittings

Flanges

Welding rods

Country

Body

Designation

USA

UNS

N08825

France

AFNOR

NC 21 FeDU

GB

BS

NA 16

Germany

DIN

NiCr21Mo

Germany

Werkstoff

Nr 2.4858

 

27-7MO 832 Alloy Seamless Pipe Specification

The chemical composition of INCOLOY alloy 27-7MO is given in the following table.

Element Content (%)
Iron, Fe 35.54-46.2
Nickel, Ni 26-28
Chromium, Cr 20.5-23
Molybdenum, Mo 6.5-8
Manganese, Mn ≤3
Others Remainder

The chemical composition INCOLOY alloy 832 is outlined in the following table.

Element Content (%)
Iron, Fe 60.645 - 70.7
Chromium, Cr 19.5 - 21
Nickel, Ni 8.75 - 15.5
Copper, Cu ≤ 0.75
Silicon, Si 0.7
Titanium, Ti 0.4
Molybdenum, Mo 0.4
Manganese, Mn 0.4
Aluminum, Al 0.15
Carbon, C ≤ 0.050
Sulfur, S ≤ 0.0050

27-7MO 832 Alloy Seamless Pipe

27-7MO 832 Alloy Seamless Pipe27-7MO 832 Alloy Seamless Pipe

27-7MO alloy is a super austenitic stainless steel containing 7% molybdenum. Compared with 6% molybdenum super austenitic stainless steel, it has better corrosion resistance in most environments. In many environments, the corrosion resistance of 27-7MO alloy is close to or even exceeds that of many superalloy materials, such as 625 alloy, 22 alloy and C-276 alloy.
Incoloy 832 is a low-cost stainless steel material developed specifically for use in sheathed heater applications in domestic and industrial applications. Suitable for use with high output banner welding machines.

 

27-7MO 832 Alloy Seamless Pipe process & size

27-7MO 832 Alloy Seamless Pipe process & size

27-7MO 832 Alloy Seamless Pipe

27-7MO 832 Alloy Seamless Pipe

 

customer visit

customer visit

27-7MO 832 Alloy Seamless Pipe

 

FAQ

Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. Or if the goods are not in stock, it is 15-20 days, depending on the quantity.

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: About the product price of 27-7MO 832 Alloy Seamless Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: 27-7mo 832 alloy seamless pipe, China 27-7mo 832 alloy seamless pipe suppliers, alloy for electron beam melting baths, alloy for repair baths, alloy for cooling baths, alloy for binder jetting baths, alloy for non magnetic materials, alloy for digital manufacturing baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry