Incoloy A-286
video

Incoloy A-286

INCOLOY® alloy A-286 (UNS S66286 / W.Nr. 1.4980) is an iron-nickel-chromium alloy with additions of molybdenum and titanium. It is agehardenable for high mechanical properties. The alloy maintains good strength and oxidation resistance at temperatures up to about 1300°F (700°C). The alloy is austenitic in all metallurgical conditions.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy a-286 in China. If you're going to wholesale high quality incoloy a-286 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy A-286 (UNS S66286 / W.Nr. 1.4980) is an iron-nickel-chromium alloy with additions of molybdenum and titanium. It is agehardenable for high mechanical properties. The alloy maintains good strength and oxidation resistance at temperatures up to about 1300°F (700°C). The alloy is austenitic in all metallurgical conditions.

The high strength and excellent fabrication characteristics of INCOLOY alloy A-286 make the alloy useful for various components of aircraft and industrial gas turbines. It is also used for fastener applications in automotive engine and manifold components subject to high levels of heat and stress and in the offshore oil and gas industry.

Mechanical Properties

In the age-hardened condition, INCOLOY alloy A-286 has high strength at room temperature and retains high levels of strength at temperatures to about 1300°F (700°C).

Mechanical properties reported here are for material given the following heat treatment: solution treatment at 1800°F (980°C) plus age hardening at 1325°F (720°C)/16 h and air cooling.

Corrosion Resistance

The nickel and chromium contents of INCOLOY alloy A-286 provide resistance to corrosion and oxidation. The alloy has excellent resistance to oxidation at service temperatures up to about 1300°F (700°C).

Main Standards

ASTM A638

Bar and Forging

SAE AMS 5726

Bar and Wire

SAE AMS 5731

Bar, Wire, Forging and Tubing

SAE AMS 5732

Bar, Wire, Forging and Tubing

SAE AMS 5734

Bar, Wire, Forging and Tubing

SAE AMS 5737

Bar, Wire, Forging and Tubing

SAE AMS 5895

Bar, Wire, Forging and Tubing

SAE AMS 5525

Plate, Sheet and Strip

SAE AMS 5858

Plate, Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 7.94
lb/in.3 0.287
Melting Range °F 2500 - 2600
°C 1370 - 1430
Specific Heat Btu/lb•°F 0.100
J/kg•°C 419
Permeability at 70°F (21°C) and 200 oersted (15.9 kA/m)   1.007

 

product-720-720product-720-720product-720-720product-720-720

 

 

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days. 

Hot Tags: incoloy a-286, China incoloy a-286 suppliers, alloy for neurology baths, lncoloy 825 plate, alloy for switches, alloy for testing baths, alloy for insulation materials, incoloy material pipe seamless

Send Inquiry

whatsapp

Phone

E-mail

Inquiry