Incoloy 800 Alloy Cold Drawn Bars
video

Incoloy 800 Alloy Cold Drawn Bars

Name:Incoloy 800 Alloy Cold Drawn Bars
Quality InspectionUt, Chemical Composition,SGS
Shape:Round/Sauqre/Flat/Hexagon
Process:Cold Drawn,Cold Rolled,Bright Anneal etc
Surface Require:Mirror Polishing, Hairline Finishing, Sb , No.4
Diameter (Od):Cold Drawn Bar:4.76~120mm(All Sizes Can Be Custom)
Application areas: Petrochemical, energy, industrial
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800 alloy cold drawn bars in China. If you're going to wholesale high quality incoloy 800 alloy cold drawn bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Ni 800 Alloy Cold Drawn Bars Description

Ni 800 Alloy Cold Drawn Bars

 

Gnee Steel Ni 800 Alloy Cold Drawn Bars

Incoloy 800 alloy cold drawn bar is a nickel-iron-chromium alloy. It has very good strength, oxidation resistance and carburization resistance in high temperature environments. The higher chromium content gives Incoloy 800 cold drawn steel bar higher oxidation resistance. It is also resistant to a variety of fluid media and generally does not suffer from stress corrosion cracking.

Size Chart of Incoloy Alloy 800 Cold Drawn Bar

Description Diameter
1.250 1.2500
1.00 1.0000
2.500 2.5000
3.00 3.0000
.500 0.5000
2.00 2.0000
2.0000 2.0000
1.500 1.5000
4.00 4.0000

Application of Incoloy 800 alloy cold drawn bar
‌Chemical equipment‌: such as heat exchangers, reactors, etc.
‌Oil and gas industry‌: used for high temperature and high pressure pipes and valves.
‌Nuclear energy industry‌: used to manufacture components for nuclear reactors.

Corrosion Resistant 800 Alloy Bar Specification

Incoloy 800 Chemical Composition of Cold Drawn Bar

Grade Ni Cr Fe Mb Ti Cu Mn C S Al Al + Ti
Incoloy 800 30.0 – 35.0 19.0 – 23.0 39.5 min – 0.15 – 0.60 – – 0.10 max – 0.15 -0.60 3.15 – 4.15

Mechanical Properties of Incoloy 800 Material Bar

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.94 g/cm3 1385 °C (2525 °F) Psi – 75,000 , MPa – 520 Psi – 30,000 , MPa – 205 30 %

Tolerance of Inconel Alloy 800 Cold Drawn Bar

Tolerance ISO "H" Series in MM
NOMINAL SIZE h8 h6 h5 h7 H10 h9 h12 H11
DIAMETER mm
over 3 to 6 +0.018/0 +0.008/0 +0.005/0 +0.012/0 +0.048/0 +0.03/0 +0.12/0 +0.075/0
~ to 3 +0.014/0 +0.006/0 +0.004/0 +0.01/0 +0.04/0 +0.025/0 +0.1/0 +0.06/0
over 6 to 10 +0.022/0 +0.009/0 +0.006/0 +0.015/0 +0.058/0 +0.036/0 +0.15/0 +0.09/0
over 18 to 30 +0.033/0 +0.013/0 +0.009/0 +0.021/0 +0.084/0 +0.052/0 +0.21/0 +0.13/0
over 180 to 250 +0.072/0 +0.029/0 +0.02/0 +0.046/0 +0.185/0 +0.115/0 +0.46/0 +0.29/0
over 10 to 18 +0.027/0 +0.011/0 +0.008/0 +0.018/0 +0.07/0 +0.043/0 +0.18/0 +0.11/0
over 30 to 50 +0.039/0 +0.016/0 +0.011/0 +0.025/0 +0.1/0 +0.062/0 +0.25/0 +0.16/0
over 80 to 120 +0.054/0 +0.022/0 +0.015/0 +0.035/0 +0.14/0 +0.087/0 +0.35/0 +0.22/0
over 50 to 80 +0.046/0 +0.019/0 +0.013/0 +0.03/0 +0.12/0 +0.074/0 +0.3/0 +0.19/0
over 120 to 180 +0.063/0 +0.025/0 +0.018/0 +0.04/0 +0.16/0 +0.1/0 +0.4/0 +0.25/0
Nickel Iron Chromium Alloy 800 Bar Testing

Nickel Iron Chromium Alloy 800 Bar Testing

Nickel Iron Chromium Alloy 800 Bar Testing

DIN 1.4876 alloy factory

 DIN 1.4876 alloy factory

DIN 1.4876 Alloy Factory

 
About Gnee Steel
Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Ni 800 Alloy Cold Drawn Bars, covering tubes: Seamless tubes: Sizes: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded tubes: Sizes: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy Round Bars Sizes: Diameter 3-800 mm;, Flat Bars Sizes: Thickness 2-100 mm; Width: 10-500 mm, Hexagonal Bars Sizes: 2-100 mm;, Wires and Extruded Profiles. We work with steel mills to provide our customers with Alloy 625 that meets or exceeds many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Ni 800 Alloy Cold Drawn Bars, Tubes, Pipes, Plates, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wire and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com