Incoloy 800 825 hot rolled seamless pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800 825 hot rolled seamless pipe in China. If you're going to wholesale high quality incoloy 800 825 hot rolled seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy Pipe Products Application
incoloy 800 825 steel pipe video
INCOLOY alloy 800 is used in the following applications:
Heat exchangers
Carburising equipment
Heating elements
Sheathing and nuclear steam generator tubing.
Applications of Incoloy 825, Nickel Alloy 825, UNS N08825
Due to its excellent corrosion resistance, Incoloy 825 is used in many industries and applications, including:
Chemical processing components
Oil and gas pipelines, recovery
Acid production
Pickling tank heaters, tanks and equipment
Marine exhaust systems
Pollution control equipment
Water heaters
Food, water and seawater thermal containers
Nuclear fuel reprocessing
Radioactive waste disposal
It is an alloy that has a high level of corrosion resistance in both moderately oxidizing and moderately reducing environments.
Incoloy Material Specification
| The Chemical Composition of Incoloy 800, % | |
|---|---|
| Ni | 30.0-35.0 |
| Cr | 19.0-23.0 |
| Fe | ≥39.5 |
| Ti | 0.15-0.60 |
| Al | 0.15-0.60 |
| C | ≤0.10 |
| Mn | ≤1.50 |
| Si | ≤1.00 |
| S | ≤0.015 |
| Cu | ≤0.75 |
Incoloy 825 Pipe Chemical Composition, %
| Grade | C≤ | Mn≤ | Si≤ | S≤ | Cu≤ | Fe(min) | Ni | Cr | Al | Ti |
| Incoloy 825 | 0.05 | 1 | 0.5 | 0.03 | 1.5-3.0 | 22 | 38.0~46.0 | 19.5~23.5 | 0.2 | 0.6-1.2 |


Incoloy 800 alloy is an iron-based alloy; it contains a large amount of Ni, Cr and a small amount of Si, Mn, Cu, Al, Ti. It has high high-temperature strength, and also has good oxidation resistance, carburization resistance and permeability resistance. Sulfur properties. High contents of Cr and Ni ensure long-term stability in corrosive environments.
Alloy 825 is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of chromium, nickel, molybdenum and copper to provide a high level of corrosion resistance in moderately oxidizing and moderately reducing environments. The alloy has high levels of nickel, which combined with the molybdenum and copper content, produce significantly improved corrosion resistance in reducing environments compared to standard stainless steel.
GNEE Group Factory Environment
Incoloy 800 825 Pipe

Customer Case
customer visit


FAQ
Q: What is your delivery time?
A: Our delivery time is about one week, based on the number of customers.
Q: How long is your delivery time?
A: This is based on quantity. Generally it is 30 days.
Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.
Q: About the product price of incoloy 800 825 pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: Incoloy 800 825 hot rolled seamless pipe, China Incoloy 800 825 hot rolled seamless pipe suppliers, incoloy material, alloy for laser sintering baths, alloy for biofabrication baths, alloy for semiconductors, alloy supplies, alloy for agile manufacturing baths
You Might Also Like
Send Inquiry