908 945 Incoloy Seamless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 908 945 incoloy seamless pipe in China. If you're going to wholesale high quality 908 945 incoloy seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
incoloy Products Application
908 945 Incoloy Seamless Pipe video
The following are the list of applications of Incoloy alloy 908:
Prototype fusion reactors
High-strength cryogenic applications.
incoloy Material Specification
| Element | Content (%) |
|---|---|
| Nickel, Ni | 47 – 51 |
| Iron, Fe | 35.588 – 44.6 |
| Chromium, Cr | 3.75 – 4.5 |
| Niobium, Nb (Columbium, Cb) | 2.7 – 3.3 |
| Titanium, Ti | 1.2 – 1.8 |
| Manganese, Mn | ≤1 |
| Aluminum, Al | 0.75 – 1.25 |
| Cobalt, Co | ≤0.50 |
| Copper, Cu | ≤0.50 |
| Silicon, Si | ≤0.50 |
| Carbon, C | ≤0.030 |
| Phosphorous, P | ≤0.015 |
| Boron, B | ≤0.012 |
| Sulfur, S | ≤0.0050 |


Incoloy 908 is an alloy based on nickel with the addition of other elements. Incoloy 908, a Monel alloy containing about 30% copper produced around 1905, is an earlier nickel alloy. Incoloy 908 nickel has good mechanical, physical and chemical properties. Adding appropriate elements can improve its oxidation resistance, corrosion resistance, high temperature strength and improve certain physical properties.
Incoloy945 Incoloy945 is a high-strength, corrosion-resistant alloy designed for demanding applications in the oil and gas industry. Contents of molybdenum, copper, niobium, titanium and aluminum enhance the properties of this age-hardenable nickel-iron-chromium alloy.
Customer Case
customer visit


FAQ
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
Q: Can I get a sample before ordering?
Answer: Yes, of course. Usually our samples are free. We can produce according to your samples or technical drawings.
Q: About the product price of 908 945 Incoloy Seamless Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.