Nickel Alloy 201 Polished Steel Plate
video

Nickel Alloy 201 Polished Steel Plate

Surface:Mirror, Brushed, Mill Finished, Polished, etc
Key Word:Nickel Alloy 201 Polished Steel Plate
Hot rolled: 3.0mm-180mm
Transport Package:Standard Seaworthy Package or Customer Requirement
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel alloy 201 polished steel plate in China. If you're going to wholesale high quality nickel alloy 201 polished steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 201 Finish Plate, also known as UNS N06600 or SAE 30001, is a nickel-chromium-molybdenum alloy that is an austenitic stainless steel with excellent mechanical properties and corrosion resistance. Similar to Nickel 200, but with a lower carbon content to help prevent high temperature embrittlement and reduce hardness. Very suitable for spinning and cold forming.


Nickel 201 also has a variety of surface treatments, Nickel 201 2B surface Finish plate, Nickel 201 mirror Finish plate, Nickel 201 #4 Finish Steel Sheet, Nickel 201 #8 Finish Steel Sheet.


Nickel 201 Thin Plate Applications
Includes alkali evaporators, combustion boats, electroplating rods, electronic components, synthetic fiber processing, food processing, heat exchange, and a variety of other applications in the chemical and electrical industries.

 

 Nickel UNS N02201 Specification

Certificate

SGS,ISO

Surface

2B,BA(bright annealed) NO.1 NO.2 NO.3 NO.4,8K HL(Hair Line) PVC

Thickness

0.15-6mm

Width

24-2000mm

Length

1-6m or as required

Delivery time

15-20 days after the deposit or LC.

Feature

Good cost performance,price stability

Good shaping capability,weld bending capability,high thermal conductivity,low thermal expansion

Shipment

Within 7-15 workdays,25-30days when the quality beyond 1000tons

 Alloys 201 Products Display

Nickel UNS N02201 Plates

Nickel UNS N02201 Plates

 

Why choosing GNEE

GNEE is currently equipped with more than 10 finishing rolling and drawing production lines and 6 electrolysis equipment. It has introduced foreign advanced equipment such as bright annealing furnaces, straighteners, internal and external fine polishing machines, ECT eddy current and ultrasonic flaw detectors and other high-end instruments, and is equipped with high-grade dust-free room.

please contact us for a quote! ss@gneesteel.com

PRODUCTS TESTING

Nickel Alloy 201 High Temperature Pipe

 Nickel 201 Heavy Duty Sheet  Exporter

Alloy 201 Black Bar Exporter

 Alloy 201 Sheet & Plate Stockists

Alloy 201 Sheet & Plate Stockists

FAQ

Q: What main products can you supply?
A: We are a professional and well-known factory in China. The main products of our company include stainless steel plates/coils/tubes/rods/corrugated sheets.
Q: How long is your delivery time?
A: Our daily inventory is more than 8000 tons, so orders of ordinary product sizes only take 5 days from stock. If there is an order for special size, it will take 7-15 days.

Hot Tags: nickel alloy 201 polished steel plate, China nickel alloy 201 polished steel plate suppliers, Hastelloy C 22 Alloy Steel Flange, Nickel Alloy Coil B2, Alloy Steel 600 plate, Uns N06600 Alloy tubing, Hastelloy C276 ROUND BAR, 2 4668 Nickel Alloy Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry