GH4169 High Strength High Temperature Alloy Bar
video

GH4169 High Strength High Temperature Alloy Bar

Specifications
Wire: 0.01-10mm
Strip: 0.05*5.0-5.0*250mm
Rod: φ4-50mm; Length 2000-5000mm
Pipe: φ6-273mm; δ1-30mm; Length 1000-8000mm
Plate: δ0.8-36mm; Width 650-2000mm; Length 800-4500mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4169 high strength high temperature alloy bar in China. If you're going to wholesale high quality gh4169 high strength high temperature alloy bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GNEE  introduce

GH4169 High strength High temperature alloy bar

GH4169 High strength High temperature alloy barGH4169 High strength High temperature alloy bar

GH4169 is a nickel-chromium-molybdenum alloy designed to resist a wide range of severe corrosive environments, pitting and crevice corrosion. This nickel steel alloy also exhibits extremely high yield, tensile and creep rupture properties at elevated temperatures. The service temperature range for this nickel alloy is from cryogenic to long term service temperatures of 1200°F.

GNEE product Chemical composition

Chemical composition of GH4169 Bar

Chemical composition(mass fraction)(wt.%) of the GH4169

Elements Min.(≥) Max.(≤)
C – 0.03
Cr 17 21
Mo 2.8 3.3
Ni 50 55
Al 0.2 0.6
Nb 4.75 5.5
Fe – Remainder
Si – 0.35
Mn – 0.35
P – 0.015
S – 0.015
B – 0.006

GNEE GH4169 high temperature alloy application

GH4169 high temperature alloy

GH4169 high temperature alloy has the characteristics of high strength, good toughness, good corrosion resistance, high high temperature stability, etc., and is widely used in aviation, aerospace, petroleum, chemical industry and other fields. In the field of aerospace, GH4169 is mainly used to manufacture high temperature parts such as turbine blades, turbine discs, combustion chambers, etc. In the field of petrochemicals, GH4169 is often used to manufacture reactors, steam generators, hydrogenation equipment, etc. In addition, GH4169 can also be used to manufacture automobile emission systems, nuclear power plant reactors and other fields.

GNEE Group Factory Environment 

GNEE Group GH4169 High temperature alloy bar Factory Environment

GH4169 High strength High temperature alloy bar

GNEE Group  Packaging 

GNEE Group GH4169 High temperature alloy bar Packaging

GH4169 High strength High temperature alloy bar

 

FAQ

Q: What's the terms of packing?
A: Generally,we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q: What's your delivery time?
A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit.
Q: Could you produce according to the samples?
A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.

Hot Tags: gh4169 high strength high temperature alloy bar, China gh4169 high strength high temperature alloy bar suppliers, Casting High Temperature Alloy