GH4098 4169 5188 Heat Resistant Metals Pipe
video

GH4098 4169 5188 Heat Resistant Metals Pipe

GH2132 is a Fe-25Ni-15Cr-based high-temperature alloy, which is comprehensively strengthened by adding molybdenum, titanium, aluminum, vanadium and trace amounts of boron.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4098 4169 5188 heat resistant metals pipe in China. If you're going to wholesale high quality gh4098 4169 5188 heat resistant metals pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GH4098 4169 5188 Heat Resistant Metals Pipe Products Description

GH4098 4169 5188 heat resistant stainless steel Pipe video


GNEE STEEL GROUP supplies GH4098 4169 5188 Heat Resistant Metals Pipe for you

 

Product Name

GH4098 Heat Resistant Metals Pipe
Outer diameter

5mm-500mm or as required

Length

2000mm-120000mm or as required

Standard

AISI,ASTM,DIN,JIS,GB,JIS,SUS,EN,etc.

Technique

Hot Rolled/Cold Rolled

Surface Treatment

Polishing,Pickling or according to customer requirement

Thickness tolerance

±0.01mm

 

GH4169 - Form of Supply

Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED

 

Prdouct Name GH 5188 Alloy
Thickness 0.1-20 mm or as requirement
Width 1000-6000 mm or as requirement
Length Customized

 

GH4098 4169 5188 Heat Resistant Metals Pipe chemical composition

GH4098 Heat Resistant Metals Pipe chemical composition

chemical Fe C Si Mn P S Cr Cu Mo Ti W Nb B Co Al Ce More
minimum value - - - - - - 17.5 - 3.5 1 5.5 - - 5 2.5 - Ni:margin
maximum value 3 0.1 0.3 0.3 0.015 0.015 19.5 0.07 5 1.5 7 1.5 0.05 8 3 0.02

GH4169 Heat Resistant Metals Pipe chemical composition

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03    
Cr 17.0 21.0    
Mo 2.80 3.30    
Ni 50.0 55.0    
Al 0.20 0.60    
Nb 4.75 5.50    
Fe - Remainder    
Si - 0.35    
Mn - 0.35    
P - 0.015    
S - 0.015    
B - 0.006    

GH5188 Heat Resistant Metals Pipe chemical composition

Element C Cr Ni Co W Fe
wt% 0.05-0.15 20.00-24.00 20.00-24.00 Bal 13.00-16.00 ≤3.00
Element B La Mn Si P S
wt% ≤0.015 0.03-0.12 ≤1.25 0.20-0.50 ≤0.02 ≤0.015
Element Cu O N – – –
wt% ≤0.07 ≤0.025 ≤0.015 – – –

GH4098 4169 5188 heat resistant metals Pipe

GH4098 4169 5188 high temperature steel alloys Pipe suppliersGH4098 4169 5188 high temperature steel Pipe price

GH4098 is a Ni-Cr-based precipitation hardening deformed high-temperature alloy with a long-term operating temperature of up to 1000°C. Elements such as tungsten, molybdenum, chromium and cobalt are added to the alloy for solid solution strengthening, elements such as aluminum, titanium and niobium are added to form a γ' phase precipitation strengthening phase, and trace amounts of boron and cerium are added for grain boundary strengthening. The comprehensive strengthening effect is obvious.
GH4169, also known as Inconel 718, is a precipitation-strengthened nickel-based high-temperature and high-strength alloy. Inconel 718 has good comprehensive properties in the temperature range of -253~700℃. The yield strength below 650℃ ranks first among deformed superalloys. It also has good fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, and good Processing performance, welding performance and long-term structural stability.
GH5188 is a solid-solution strengthened cobalt-based high-temperature alloy. Adding 14% tungsten solid-solution strengthening gives the alloy excellent high-temperature thermal strength. Adding a higher content of chromium and trace amounts of lanthanum gives the alloy good high-temperature oxidation resistance. It has satisfactory process properties such as forming and welding, and is suitable for manufacturing parts for aero engines that require high strength below 980°C and oxidation resistance below 1100°C.

 

Product technology

 

GH4098 4169 5188 Heat Resistant Metals Pipe

GH4098 4169 5188 Heat Resistant Metals Pipe

 

 

Customer Case

customer visit

GH4098 4169 5188 Heat Resistant Metals Pipe

FAQ

Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.

Q: Can I get your best price?
A: Our goal is to provide you with the best price and excellent quality assurance in the long run. Please leave your contact information to get the best quote, we will provide you with the best solution as soon as possible.

Q: About the product price of GH4098 4169 5188 high heat stainless steel?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: gh4098 4169 5188 heat resistant metals pipe, China gh4098 4169 5188 heat resistant metals pipe suppliers, Casting High Temperature Alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry